Friday, February 24, 2012

[MW:13776] SS welding with SAW

Dear Experts,
Could anyone suggest me about the followings for stainless steel SAW welding to reach >0.38mm %LE at -196deg. cen.

 

  1. Limitation of wire composition for ER308L grade wire.
  2. SAW welding parameters. (A/V/Speed)
  3. Preheating & Heat input for more than 50mm thick plate.
  4. Any other special requirement.

 

Rgd