Iwhat is the meninig of IQS Thanks & Regards,
K.GANESAN Quality Control ISGEC / ISGEC John Thompson, A-4 Sector-24 Noida-201301 (UP) Tel. +91-120-2411175 Direct Tel. +91-120-2411175 Mobile : +91-9952166894
--- On Tue, 28/7/09, SLM <smahuri@lntecc.com> wrote: From: SLM <smahuri@lntecc.com> Subject: [MW:2829] RE: 2827] AWS-CWI best agency in INDIA To: materials-welding@googlegroups.com Date: Tuesday, 28 July, 2009, 9:20 AM
Yes, you have rightly heard. Among the four listed agencies IQC is the best. As most of my friends have completed this course successfully through IQC only. So you can opt for IQC. Thanks and Regards, Snehkumar L Mahuri Regional Quality Manager HC&P (Vertical) M : 9428819849 From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of PREMSHANKARDUTTNAUTIYAL Sent: Tuesday, July 28, 2009 9:04 AM To: materials-welding@googlegroups.com Subject: [MW:2827] AWS-CWI best agency in INDIA Hi Friends
I stay in Mumbai and have prepared for AWS-CWI and want to appear for Course + Exam in the next couple of months. But in India there are 4 AWS approved agencies which conduct this AWS course.I am confused as to which agency i should select as i have to invest a huge amount of money... .
1)Industrial Quality Concepts Address: IQC Training & Services, Pte, Ltd Shivani Block -1, Ist Floor 40 East Coast Road Chennai, India 600041 Telephone: 91-44-42158714/42158715/24451009 Fax Number: 91-44-5215-8715 Email: iqc.in.org@vsnl.com Contacts: Sundaran Baskaran
2)BETZ Engineering & Technology Zone Address: 49-Vellalar Street Near St Thomas Mount Railway Station Chennai - 600088 INDIA Tel: 91-44-65364123/22441234 TeleFax: 91-44-22441234 Email: betzzone@vsnl.net Site: www.betzinternational.com
3)DASH Inspectorate Address: 3rd Floor,Iswar Krupa Building Near Bank Of India, Saffron Circle,Fatehgunj, Baroda-390002,Gujarat,India Phone: +91 265 2750116, 3017474 Fax: +91 265 2788278 Site: www.dashinspectorate.com
4)Agency: Moody ICL Certifications Limited Address: #372, Industrial Area Phase I Panchkula Haryana India PIN 134112 Website: www.moodyint.com
Hence can anyone guide me from their past experience as to which agency is the best. Please give your unbiased opinion.. I have heard from all my colleagues that IQC,chennai is the best and most experienced in conducting CWI.
Please guide me to select the best agency which will provide good preparatory training.
Regards
Prem Nautiyal Mumbai.
PREM S NAUTIYAL
CELL : 9820313278 </Table
| "This Message and its contents is intended solely for the addressee and is proprietary.Information in this mail is for L&T Business Usage only. Any Use to other than the addressee is misuse and infringement to Proprietorship of L&T ECC.If you are not the addressee please return the mail to the sender.L&T ECC DIVISION"
See the Web's breaking stories, chosen by people like you. Check out Yahoo! Buzz --~--~---------~--~----~------------~-------~--~----~ To post to this group, send email to materials-welding@googlegroups.com To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com For more options, visit this group's bolg at http://materials-welding.blogspot.com/ The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents. -~----------~----~----~----~------~----~------~--~---
Your understanding is correct. It is exempted From: Vivek Bhisade [mailto:vivek@tpr.grengg.com] Sent: Tuesday, July 28, 2009 2:20 PM To: materials-welding@googlegroups.com Subject: Toughness Requirement for Dissimiller Weld Dear All, We have a job ( hydro generator) material SA 387 Gr.11 CL 2 + SS347 ( clad) ,required impact testing at (minus)-18 Deg.C with energy value 33 J average (irrespective of MDMT ),having some nozzles (LWNR) material is SA 182 F 347. For Welding Procedure Qualification of Dissimilar metals Nozzle to Shell joint ( P4 To P8) using electrodes by E309L , weld Impact test is required or not? As per ASME SEC VIII Div 1 – UHA-51 (e) it is exempted , Please advise. Thanks in advance. --~--~---------~--~----~------------~-------~--~----~ To post to this group, send email to materials-welding@googlegroups.com To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com For more options, visit this group's bolg at http://materials-welding.blogspot.com/ The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents. -~----------~----~----~----~------~----~------~--~---
Dear All, We have a job ( hydro generator) material SA 387 Gr.11 CL 2 + SS347 ( clad) ,required impact testing at (minus)-18 Deg.C with energy value 33 J average (irrespective of MDMT ),having some nozzles (LWNR) material is SA 182 F 347. For Welding Procedure Qualification of Dissimilar metals Nozzle to Shell joint ( P4 To P8) using electrodes by E309L , weld Impact test is required or not? As per ASME SEC VIII Div 1 – UHA-51 (e) it is exempted , Please advise. Thanks in advance. --~--~---------~--~----~------------~-------~--~----~ To post to this group, send email to materials-welding@googlegroups.com To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com For more options, visit this group's bolg at http://materials-welding.blogspot.com/ The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents. -~----------~----~----~----~------~----~------~--~---
Dear Ali, If you are looking at an international company that undertakes failure investigations , you can count on TCR Engineering Services and our sister concern TCR Advanced Engineering based in India. We have done over 800 failure investigations, RLA and Condition Assessment on various metallic components related to almost all the engineering fields over past one decade. Please visit our website at www.tcreng.com to know more about our FA services. Regards, Rohit Bafna Director - Global Sales ------------------------------------------ TCR Engineering Services (India) TCR Arabia (KSA), TCR Kuwait TCR Consulting FZC (UAE) TCR Nigeria, TCR Malaysia TCR World Inc. (USA) India Tel: +91-983-353-0400 www.tcreng.com Material Testing | Consulting | Inspection | NDT Services ------------------------------------------- From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of Ali Asghari Sent: Monday, July 27, 2009 11:13 PM To: materials-welding@googlegroups.com Subject: [MW:2831] CEA COURSE does anybody have information about international certificates & organizations about failure investigation or critical engineering assessment and fracture mechanics?
--~--~---------~--~----~------------~-------~--~----~ To post to this group, send email to materials-welding@googlegroups.com To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com For more options, visit this group's bolg at http://materials-welding.blogspot.com/ The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents. -~----------~----~----~----~------~----~------~--~---
Dear Friends The IITs have taken up an initiative of starting online teaching and thus > have started offering course materials online for every engineering > stream. > Many professors from all the IITs have provided course materials for each > chapter and each subject.. > > One has to register at the link provided below and can access the course > material free of cost. > > Every Chapter has been described with diagrams and charts. Please spread > this message to everyone, as many can benefit from this program taken up > by the government and IIT. > > This is just a trial period going on and hence I request everyone to > register at the link given. > > 1] Type the following address on internet explorer > http://www.nptel.iitm.ac.in > > 2] Click on Courses and one can access any course material. > > Please spread the word, so that this initiative benefits as many Students > as possible. > > Regards > > Prem Nautiyal Godrej,Mumbai > PREM S NAUTIYAL CELL : 9820313278 --~--~---------~--~----~------------~-------~--~----~ To post to this group, send email to materials-welding@googlegroups.com To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com For more options, visit this group's bolg at http://materials-welding.blogspot.com/ The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents. -~----------~----~----~----~------~----~------~--~---
HI All, It all depends upon the tutor and the materials which he gives during the class. Regards, Y.C.Shiva, QA/QC Engineer, Certified Inspector API 653,570, CSWIP 3.1, NACE CIP lev 2, Doha Qatar. On 7/28/09, SLM <smahuri@lntecc.com> wrote: > Yes, you have rightly heard. > > Among the four listed agencies IQC is the best. As most of my friends have > completed this course successfully through IQC only. > So you can opt for IQC. > > > Thanks and Regards, > > Snehkumar L Mahuri > Regional Quality Manager > HC&P (Vertical) > > M : 9428819849 > > From: materials-welding@googlegroups.com > [mailto:materials-welding@googlegroups.com] On Behalf Of > PREMSHANKARDUTTNAUTIYAL > Sent: Tuesday, July 28, 2009 9:04 AM > To: materials-welding@googlegroups.com > Subject: [MW:2827] AWS-CWI best agency in INDIA > > Hi Friends > > I stay in Mumbai and have prepared for AWS-CWI and want to appear for Course > + Exam in the next couple of months. But in India there are 4 AWS approved > agencies which conduct this AWS course.I am confused as to which agency i > should select as i have to invest a huge amount of money... . > > 1)Industrial Quality Concepts > Address: IQC Training & Services, Pte, Ltd > Shivani Block -1, Ist Floor > 40 East Coast Road > Chennai, India 600041 > Telephone: 91-44-42158714/42158715/24451009 > Fax Number: 91-44-5215-8715 > Email: iqc.in.org@vsnl.com > Contacts: Sundaran Baskaran > > 2)BETZ Engineering & Technology Zone > Address: 49-Vellalar Street > Near St Thomas Mount Railway Station > Chennai - 600088 > INDIA > Tel: 91-44-65364123/22441234 > TeleFax: 91-44-22441234 > Email: betzzone@vsnl.net > Site: www.betzinternational.com > > 3)DASH Inspectorate > Address: 3rd Floor,Iswar Krupa Building Near Bank Of India, > Saffron Circle,Fatehgunj, > Baroda-390002,Gujarat,India > Phone: +91 265 2750116, 3017474 > Fax: +91 265 2788278 > Site: www.dashinspectorate.com > > 4)Agency: Moody ICL Certifications Limited > Address: #372, Industrial Area Phase I > Panchkula > Haryana > India > PIN 134112 > Website: www.moodyint.com > > Hence can anyone guide me from their past experience as to which agency is > the best. Please give your unbiased opinion.. > I have heard from all my colleagues that IQC,chennai is the best and most > experienced in conducting CWI. > > Please guide me to select the best agency which will provide good > preparatory training. > > Regards > > Prem Nautiyal > Mumbai. > > PREM S NAUTIYAL > > CELL : 9820313278 > [http://sigads.rediff.com/RealMedia/ads/adstream_nx.ads/www.rediffmail.com/signatureline.htm@Middle]<http://sigads.rediff.com/RealMedia/ads/click_nx.ads/www.rediffmail.com/signatureline.htm@Middle?></Table > > > > > > ________________________________ > "This Message and its contents is intended solely for the addressee and is > proprietary.Information in this mail is for L&T Business Usage only. Any Use > to other than the addressee is misuse and infringement to Proprietorship of > L&T ECC.If you are not the addressee please return the mail to the > sender.L&T ECC DIVISION" > > > > --~--~---------~--~----~------------~-------~--~----~ To post to this group, send email to materials-welding@googlegroups.com To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com For more options, visit this group's bolg at http://materials-welding.blogspot.com/ The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents. -~----------~----~----~----~------~----~------~--~---
Hi all does anybody have information about international certificates & organizations about failure investigation or critical engineering assessment and fracture mechanics? regards. --~--~---------~--~----~------------~-------~--~----~ To post to this group, send email to materials-welding@googlegroups.com To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com For more options, visit this group's bolg at http://materials-welding.blogspot.com/ The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents. -~----------~----~----~----~------~----~------~--~---
Hi every body, Can anyone send me old/model question papers for API 570 exam. I hope this will be useful for many aspirants. __________ Information from ESET NOD32 Antivirus, version of virus signature database 4283 (20090727) __________ The message was checked by ESET NOD32 Antivirus. http://www.eset.com --~--~---------~--~----~------------~-------~--~----~ To post to this group, send email to materials-welding@googlegroups.com To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com For more options, visit this group's bolg at http://materials-welding.blogspot.com/ The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents. -~----------~----~----~----~------~----~------~--~---
Yes, you have rightly heard. Among the four listed agencies IQC is the best. As most of my friends have completed this course successfully through IQC only. So you can opt for IQC. Thanks and Regards, Snehkumar L Mahuri Regional Quality Manager HC&P (Vertical) M : 9428819849 From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of PREMSHANKARDUTTNAUTIYAL Sent: Tuesday, July 28, 2009 9:04 AM To: materials-welding@googlegroups.com Subject: [MW:2827] AWS-CWI best agency in INDIA Hi Friends I stay in Mumbai and have prepared for AWS-CWI and want to appear for Course + Exam in the next couple of months. But in India there are 4 AWS approved agencies which conduct this AWS course.I am confused as to which agency i should select as i have to invest a huge amount of money... . 1)Industrial Quality Concepts Address: IQC Training & Services, Pte, Ltd Shivani Block -1, Ist Floor 40 East Coast Road Chennai, India 600041 Telephone: 91-44-42158714/42158715/24451009 Fax Number: 91-44-5215-8715 Email: iqc.in.org@vsnl.com Contacts: Sundaran Baskaran 2)BETZ Engineering & Technology Zone Address: 49-Vellalar Street Near St Thomas Mount Railway Station Chennai - 600088 INDIA Tel: 91-44-65364123/22441234 TeleFax: 91-44-22441234 Email: betzzone@vsnl.net Site: www.betzinternational.com 3)DASH Inspectorate Address: 3rd Floor,Iswar Krupa Building Near Bank Of India, Saffron Circle,Fatehgunj, Baroda-390002,Gujarat,India Phone: +91 265 2750116, 3017474 Fax: +91 265 2788278 Site: www.dashinspectorate.com 4)Agency: Moody ICL Certifications Limited Address: #372, Industrial Area Phase I Panchkula Haryana India PIN 134112 Website: www.moodyint.com Hence can anyone guide me from their past experience as to which agency is the best. Please give your unbiased opinion.. I have heard from all my colleagues that IQC,chennai is the best and most experienced in conducting CWI. Please guide me to select the best agency which will provide good preparatory training. Regards Prem Nautiyal Mumbai. PREM S NAUTIYAL CELL : 9820313278  |
</Table | "This Message and its contents is intended solely for the addressee and is proprietary.Information in this mail is for L&T Business Usage only. Any Use to other than the addressee is misuse and infringement to Proprietorship of L&T ECC.If you are not the addressee please return the mail to the sender.L&T ECC DIVISION" --~--~---------~--~----~------------~-------~--~----~ To post to this group, send email to materials-welding@googlegroups.com To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com For more options, visit this group's bolg at http://materials-welding.blogspot.com/ The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents. -~----------~----~----~----~------~----~------~--~---
IQC is the oldest one in India, and I have no comments on the rest, anyway don’t worry much as industry colleagues says this one is difficult to fail (sorry nothing to degrade this exam but its moral booster to all who ever is appearing), it just basic knowledge on welding fundamentals are required. From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of PREMSHANKARDUTTNAUTIYAL Sent: Tuesday, July 28, 2009 9:04 AM To: materials-welding@googlegroups.com Subject: [MW:2827] AWS-CWI best agency in INDIA Hi Friends I stay in Mumbai and have prepared for AWS-CWI and want to appear for Course + Exam in the next couple of months. But in India there are 4 AWS approved agencies which conduct this AWS course.I am confused as to which agency i should select as i have to invest a huge amount of money... . 1)Industrial Quality Concepts Address: IQC Training & Services, Pte, Ltd Shivani Block -1, Ist Floor 40 East Coast Road Chennai, India 600041 Telephone: 91-44-42158714/42158715/24451009 Fax Number: 91-44-5215-8715 Email: iqc.in.org@vsnl.com Contacts: Sundaran Baskaran 2)BETZ Engineering & Technology Zone Address: 49-Vellalar Street Near St Thomas Mount Railway Station Chennai - 600088 INDIA Tel: 91-44-65364123/22441234 TeleFax: 91-44-22441234 Email: betzzone@vsnl.net Site: www.betzinternational.com 3)DASH Inspectorate Address: 3rd Floor,Iswar Krupa Building Near Bank Of India, Saffron Circle,Fatehgunj, Baroda-390002,Gujarat,India Phone: +91 265 2750116, 3017474 Fax: +91 265 2788278 Site: www.dashinspectorate.com 4)Agency: Moody ICL Certifications Limited Address: #372, Industrial Area Phase I Panchkula Haryana India PIN 134112 Website: www.moodyint.com Hence can anyone guide me from their past experience as to which agency is the best. Please give your unbiased opinion.. I have heard from all my colleagues that IQC,chennai is the best and most experienced in conducting CWI. Please guide me to select the best agency which will provide good preparatory training. Regards Prem Nautiyal Mumbai. PREM S NAUTIYAL CELL : 9820313278 --~--~---------~--~----~------------~-------~--~----~ To post to this group, send email to materials-welding@googlegroups.com To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com For more options, visit this group's bolg at http://materials-welding.blogspot.com/ The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents. -~----------~----~----~----~------~----~------~--~---
Hi Friends I stay in Mumbai and have prepared for AWS-CWI and want to appear for Course + Exam in the next couple of months. But in India there are 4 AWS approved agencies which conduct this AWS course.I am confused as to which agency i should select as i have to invest a huge amount of money... . 1)Industrial Quality Concepts Address: IQC Training & Services, Pte, Ltd Shivani Block -1, Ist Floor 40 East Coast Road Chennai, India 600041 Telephone: 91-44-42158714/42158715/24451009 Fax Number: 91-44-5215-8715 Email: iqc.in.org@vsnl.com Contacts: Sundaran Baskaran 2)BETZ Engineering & Technology Zone Address: 49-Vellalar Street Near St Thomas Mount Railway Station Chennai - 600088 INDIA Tel: 91-44-65364123/22441234 TeleFax: 91-44-22441234 Email: betzzone@vsnl.net Site: www.betzinternational.com 3)DASH Inspectorate Address: 3rd Floor,Iswar Krupa Building Near Bank Of India, Saffron Circle,Fatehgunj, Baroda-390002,Gujarat,India Phone: +91 265 2750116, 3017474 Fax: +91 265 2788278 Site: www.dashinspectorate.com 4)Agency: Moody ICL Certifications Limited Address: #372, Industrial Area Phase I Panchkula Haryana India PIN 134112 Website: www.moodyint.com Hence can anyone guide me from their past experience as to which agency is the best. Please give your unbiased opinion.. I have heard from all my colleagues that IQC,chennai is the best and most experienced in conducting CWI. Please guide me to select the best agency which will provide good preparatory training. Regards Prem Nautiyal Mumbai. PREM S NAUTIYAL CELL : 9820313278 --~--~---------~--~----~------------~-------~--~----~ To post to this group, send email to materials-welding@googlegroups.com To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com For more options, visit this group's bolg at http://materials-welding.blogspot.com/ The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents. -~----------~----~----~----~------~----~------~--~---  |
Hi Joel, its been a while since you taught my manufacturing processes class (the one we did semiautomatic SAW). I'm happy to help. The answers are below and my company is in the signature. 1. No 2. Heavy Fabrication 3. Indoor Regards,
Dale Jones Welding Engineer & CWI Fisher Controls, Emerson Process Management Marshaltown, IA 50158
--- On Wed, 7/15/09, Armstrong, Joel <JoelArmstrong@letu.edu> wrote:
From: Armstrong, Joel <JoelArmstrong@letu.edu> Subject: [MW:2691] Safety Question To: materials-welding@googlegroups.com Date: Wednesday, July 15, 2009, 9:04 AM
All, I work for LeTourneau Technologies and we build some of the world's largest front end loaders and jack-up drilling rigs. Obviously, we're a heavy fabrication facility. Our Safety department has been asked to investigate the need of wearing hard hats in all manufacturing areas. This would include assembly, machining, heat treat, cutting, as well as welding. Our GM of Fabrication and Assembly has asked me to get a survey of other companies' policies on the wearing of hard hats. So, if you could respond and let me know the following. 1. Does your company require manufacturing personnel to wear hard hats? 2. What type of industry are you in a. Heavy Fabrication b. Sheet Metal / Automotive c. Construction d. Wholesale Trade e. Cutting f. Other (Please specify) 3. Does your manufacturing/operations primarily take place... indoors or outdoors. 4. What is the name of your company. 5. What country is your facility located? Also, if you have recently changed companies or know for sure the policies of a facility other than your current location, feel free to answer the survey from that point of view as well. Thanks, Joel Armstrong, CWI Welding Engineer LeTourneau Technologies Member AWS B1 Committee --~--~---------~--~----~------------~-------~--~----~ To post to this group, send email to materials-welding@googlegroups.com To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com For more options, visit this group's bolg at http://materials-welding.blogspot.com/ The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents. -~----------~----~----~----~------~----~------~--~---
Hi As its %elongation is very low Better try buttering on jt surrace with ductile consumable like pure Ni i. E Ni1 And later weld jt with c...
-
Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? ...
-
Definition of buttering from ASME Section IX, QW/QB-492 Definitions: Buttering: the addition of material, by welding, on one or bot...
-
Section I. PRINT READING 3-1. GENERAL a. Drawings . Drawing or sketching is a universal language used to convey all necessary information to...
|
|