This is a specialty filler metal, 1¼Cr-½Mo base with the addition of vanadium and high carbon content (relative to most filler metals). This material does not conform to any AWS/ASME classification. Typical applications are listed in the US Welding Corp. literature. See: http://www.usweldingcorp.com/TDS/tds6458.pdf
It is used for welding and repair of similar materials in turbines etc.
John A. Henning
Welding & Materials
From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of Roy LIU??
Sent: Monday, February 20, 2012 12:49 AM
To: materials-welding@googlegroups.com
Subject: [MW:13746] TURBALOY® 17-22 (US WELDING)
Hi, Experts,
Could anyone teach me what the TURBALOY® 17-22 material is?
I can not find the proper AWS code for this material.
this datasheet shows us nothing! (below link)
http://usweldingcorp.com/MSDS/6458.pdf
Thanks!!
Best regards
Roy
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
______________________________________________________________________
The information in this email is confidential, and is intended solely for the addressee(s). If you are not the intended recipient of this email please let us know by reply and then delete it from your system; you should not copy this message or disclose its contents to anyone. The internet can not guarantee the integrity of this message. HAMON (and its subsidiaries) shall (will) not therefore be liable for the message if modified.
______________________________________________________________________
Comments