Dear Experts,
 
Good day to all. I have 2 cases which are to be shared with you for my knowledge.
 
(1) I have qualified a WPS of 8.5 mm. Base metal Thk. of P-1 G-1 to G-2. Root Run TIG and subsequent SMAW. TIG weld deposit thk. 2.5 mm. and SMAW weld deposit thk. 6 mm. PWHT- Normalizing and Tempering with Impact test at MDMT (-45º C.)
 
As per my opinion, as per QW-403.6- Minm. T qualified shall be 1.5 mm. & Max. will be 9.35 mm. as per QW-407.4. As per QW 451.1 qualified deposited weld metal thk. range will be 2t (viz. 5 mm. for TIG and 12 mm. for SMAW.) for groove welding. and for Fillet- deposited weld metal thk. range will be all fillet size. Am I correct?
 
(2) I shall have to qualify a WPS of 6 mm. Base metal Thk. (T) of P No. 8 Group 1 to itself. Complete TIG. 
 
As per my opinion, QW-202.4 (b) (1) and QW-451.1 Min Qualified T shall be 1.5 mm. and no limitation on Max. T qualified. As per QW 451.1 qualified deposited weld metal thk. range will be max. unlimited for groove welding. and for Fillet- deposited weld metal thk. range will be all fillet size. Am I correct?
 
Please share your experience with me on urgent basis.
 
Thanks & regards,
 
C. R. GANDHI
(Manager- Q. C.)
 
  
 
 
 
 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:35754] interpration

  Interpretation #: BPV IX-18-34  Record Number: 18-771  Subject Description: SC IX; QW-401.1 and QW-403.6 - Thickness Range Qualified for I...