Monday, June 27, 2022

[MW:33191] Re: Welding Process for Rail Material A75 ( DIN 536)

Dear Vinu ,  
please  refe tthe AWS standard / ISO standrds for this  flash but welding / thermit welding of rails  

AWS D15.2/D15.2M- Recommended Practices for the Welding of Rails and Related Rail Components for Use by Rail Vehicles to get some basic idea about qualification  and ask your cleint are they having project specifcations for  rail welding.
type of tests required for any welding procedure will be confimed by welding code , contrsctuintion code& project specifications& recommended practices applicable for a project .

common test fro rail welds are 
NDT - RT/ UT(PREFERABLE) , MT
weld chemistry 
macro
hardness
metallurgucal test
bend test 
TRANSFER TESTS  
 MICRO (METALLURGYCIAL ANALYSIS )

Thanks & regards, 
Srinivas Rao

On Sunday, June 26, 2022 at 5:57:52 PM UTC+4 vinu raveendran wrote:
Dear Rao,
Thanks for the advise.

Can you please share as per which code we need to do a PQR coupon  and what mechanical/ NDT tests need to perform for qualifying WPS. 

On Sunday, June 26, 2022 at 9:23:47 AM UTC+3 srinivas rao wrote:

Dear Vinu,
Most commonly used welding process's for  rail welding is 
1. Flash butt welding process  
2. Thermit welding process 

Regards,
Srinivasarao
Welding engineer , GPS 
On Friday, June 24, 2022 at 2:31:50 PM UTC+4 vinu raveendran wrote:
Dear Experts,

Please advise what welding process is recommended to join rail material A75 (DIN 356) and as per which reference code/standard. Also mention what NDT to be performed.

--
VINU RAVEENDRAN

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/dea5e5a2-f451-4530-b098-d4f743429368n%40googlegroups.com.

Re: [MW:33190] RE: PWHT Segment Wise for 9 Meter Dia Vessel

Dear Jayakumar
Not exactly. UW 4-(a)(8) covers everything else. As i mentioned it is not a preferable/recommended method (either go with Modular or Internal firing are most appropriate). 

"provided that other measures (based upon sufficiently similar, documented experience or evaluation) are taken that consider the effect of thermal gradients,
all significant structural discontinuities (such as nozzles, attachments, head to shell junctures), and any mechanical loads which may be present during PWHT.
The portion of the vessel or component outside the soak band shall be protected so that the temperature gradient is not harmful".


On Sun, 26 Jun 2022 at 11:55, 'james gerald' via Materials & Welding <materials-welding@googlegroups.com> wrote:
Dear Raghuram,

Just for knowledge purpose. Do ASME Sec.VIII Div.I the applicable code permit LOCAL PWHT of Longitudinal seams.



Thanks & Regards

J.Gerald Jayakumar




On Sunday, 26 June, 2022 at 07:46:29 am GMT+4, Raghuram Bathula <raghurambathula@gmail.com> wrote:


Although no restriction in code preferable methoud could custom build modular furnace (with panel construction) at site

It is straight forward method for cir seams, however for long seams you have to work a methodology for placing coils locally using WRC 452 guidelines, probably  supplimented with an FEA to check thermal stresses

On Sat, Jun 25, 2022, 8:21 PM <pgoswami@rogers.com> wrote:

Hi,

It's allowed by Sec VIII, DIV1. Please see the highlighted clauses as below.

Thanks.

 

Pradip Goswami.P.Eng, IWE.

Independent Welding & Metallurgical Engineering Specialist

Saudi Aramco Approved Designated Project Welding Engineer (DPWR)

Qatar Petroleum Approved, SME-Materials & Corrosion Engineering.

Linkedin: https://www.linkedin.com/in/pradip-goswami-2999855/

Email:pgoswami@rogers.com,pradip.goswami@gmail.com

Cell/Whasapp:1-905-9793232

 

UW-40 PROCEDURES FOR POSTWELD HEAT TREATMENT:

From: vishal hirde <vishalhirde1988@gmail.com>
Sent: June 25, 2022 8:24 AM
To: materials-welding@googlegroups.com
Subject: PWHT Segment Wise for 9 Meter Dia Vessel

 

Dear All,

 

We are fabricating a Vessel of Diameter 9 Meter at Site, requires PWHT: Material Grade SA 516 Gr. 70.

 

 For Circumferential Joint PWHT can it be performed Segment Wise as diameter is more??

 

Pl. Confirm as per ASME Sec VIII Div 1 can it be done in Segment Wise. 

 

--

With Best Regards,

Vishal Hirde




---

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CADxVubnaK4qDatj9JENMwNGPw7AZOFa%2BcCg4r9HrRPYDqc86Ew%40mail.gmail.com.

Re: [MW:33189] RE: PWHT Segment Wise for 9 Meter Dia Vessel

Thank You Experts for Valuable Comments.

As per discussion in trailing mail, Conclusion: as per Code localized PWHT Segment Wise using Induction Coil Heating Method can be considered for this Job.

Regards,

VH


On Sun, Jun 26, 2022 at 1:06 PM 'james gerald' via Materials & Welding <materials-welding@googlegroups.com> wrote:
Straight to the point Mr. Vishwas.

Thanks & Regards

J.Gerald Jayakumar



On Sunday, 26 June, 2022 at 10:54:11 am GMT+4, Vishwas Keskar <vvkeskar123@gmail.com> wrote:


Dear Vishal 
As I understand  correctly , the vessel circumference is 9 mtr  and  your query is that you want to carry out the PWHT of the Circumferemtial seam in segments.

The answer is No . You have to carry out PWHT  of  ENTIRE Circumferencial joint in ONE cycle.
You can do it by LOCAL PWHT method by wrapping Electric Resitance Coil on job and attaching job thermocouples.

Many HT contracter are doing such type jobs regularly.
Thanks 
Vishwas Keskar 
IWE- International Welding Enginner

On Sat, 25 Jun 2022, 20:21 , <pgoswami@rogers.com> wrote:

Hi,

It's allowed by Sec VIII, DIV1. Please see the highlighted clauses as below.

Thanks.

 

Pradip Goswami.P.Eng, IWE.

Independent Welding & Metallurgical Engineering Specialist

Saudi Aramco Approved Designated Project Welding Engineer (DPWR)

Qatar Petroleum Approved, SME-Materials & Corrosion Engineering.

Linkedin: https://www.linkedin.com/in/pradip-goswami-2999855/

Email:pgoswami@rogers.com,pradip.goswami@gmail.com

Cell/Whasapp:1-905-9793232

 

UW-40 PROCEDURES FOR POSTWELD HEAT TREATMENT:

From: vishal hirde <vishalhirde1988@gmail.com>
Sent: June 25, 2022 8:24 AM
To: materials-welding@googlegroups.com
Subject: PWHT Segment Wise for 9 Meter Dia Vessel

 

Dear All,

 

We are fabricating a Vessel of Diameter 9 Meter at Site, requires PWHT: Material Grade SA 516 Gr. 70.

 

 For Circumferential Joint PWHT can it be performed Segment Wise as diameter is more??

 

Pl. Confirm as per ASME Sec VIII Div 1 can it be done in Segment Wise. 

 

--

With Best Regards,

Vishal Hirde




AVG logo

This email has been checked for viruses by AVG antivirus software.
www.avg.com


--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/!%26!AAAAAAAAAAAuAAAAAAAAABVPzeizzeRJsiPziIE5jXQBAMO2jhD3dRHOtM0AqgC7tuYAAAAAAA4AABAAAAD9ib%2BzVU4dRb/ePF01LBnGAQAAAAA%3D%40rogers.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CADder3Pk96%3DsLj8Qgn%2B17h7%2B5A3t7bYEJKFGBnBcm4b4kO7tRA%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/2053801785.4862984.1656227327732%40mail.yahoo.com.


--
With Best Regards,

Vishal Hirde
Inspection Engineer
Velosi Certification Services (I) Pvt Ltd




--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CACAaqdoig20b5UQKpAOE9CDf3Dd9e_3ZCD%2B-xksoDCYD7bre7A%40mail.gmail.com.

Sunday, June 26, 2022

[MW:33187] Re: Welding Process for Rail Material A75 ( DIN 536)

Dear Rao,
Thanks for the advise.

Can you please share as per which code we need to do a PQR coupon  and what mechanical/ NDT tests need to perform for qualifying WPS. 

On Sunday, June 26, 2022 at 9:23:47 AM UTC+3 srinivas rao wrote:

Dear Vinu,
Most commonly used welding process's for  rail welding is 
1. Flash butt welding process  
2. Thermit welding process 

Regards,
Srinivasarao
Welding engineer , GPS 
On Friday, June 24, 2022 at 2:31:50 PM UTC+4 vinu raveendran wrote:
Dear Experts,

Please advise what welding process is recommended to join rail material A75 (DIN 356) and as per which reference code/standard. Also mention what NDT to be performed.

--
VINU RAVEENDRAN

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/8169d4ca-152f-4f16-8b73-6fe4a67e22e1n%40googlegroups.com.

Re: [MW:33185] RE: PWHT Segment Wise for 9 Meter Dia Vessel

Straight to the point Mr. Vishwas.

Thanks & Regards

J.Gerald Jayakumar



On Sunday, 26 June, 2022 at 10:54:11 am GMT+4, Vishwas Keskar <vvkeskar123@gmail.com> wrote:


Dear Vishal 
As I understand  correctly , the vessel circumference is 9 mtr  and  your query is that you want to carry out the PWHT of the Circumferemtial seam in segments.

The answer is No . You have to carry out PWHT  of  ENTIRE Circumferencial joint in ONE cycle.
You can do it by LOCAL PWHT method by wrapping Electric Resitance Coil on job and attaching job thermocouples.

Many HT contracter are doing such type jobs regularly.
Thanks 
Vishwas Keskar 
IWE- International Welding Enginner

On Sat, 25 Jun 2022, 20:21 , <pgoswami@rogers.com> wrote:

Hi,

It's allowed by Sec VIII, DIV1. Please see the highlighted clauses as below.

Thanks.

 

Pradip Goswami.P.Eng, IWE.

Independent Welding & Metallurgical Engineering Specialist

Saudi Aramco Approved Designated Project Welding Engineer (DPWR)

Qatar Petroleum Approved, SME-Materials & Corrosion Engineering.

Linkedin: https://www.linkedin.com/in/pradip-goswami-2999855/

Email:pgoswami@rogers.com,pradip.goswami@gmail.com

Cell/Whasapp:1-905-9793232

 

UW-40 PROCEDURES FOR POSTWELD HEAT TREATMENT:

From: vishal hirde <vishalhirde1988@gmail.com>
Sent: June 25, 2022 8:24 AM
To: materials-welding@googlegroups.com
Subject: PWHT Segment Wise for 9 Meter Dia Vessel

 

Dear All,

 

We are fabricating a Vessel of Diameter 9 Meter at Site, requires PWHT: Material Grade SA 516 Gr. 70.

 

 For Circumferential Joint PWHT can it be performed Segment Wise as diameter is more??

 

Pl. Confirm as per ASME Sec VIII Div 1 can it be done in Segment Wise. 

 

--

With Best Regards,

Vishal Hirde




AVG logo

This email has been checked for viruses by AVG antivirus software.
www.avg.com


--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/!%26!AAAAAAAAAAAuAAAAAAAAABVPzeizzeRJsiPziIE5jXQBAMO2jhD3dRHOtM0AqgC7tuYAAAAAAA4AABAAAAD9ib%2BzVU4dRb/ePF01LBnGAQAAAAA%3D%40rogers.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CADder3Pk96%3DsLj8Qgn%2B17h7%2B5A3t7bYEJKFGBnBcm4b4kO7tRA%40mail.gmail.com.

Re: [MW:33181] RE: PWHT Segment Wise for 9 Meter Dia Vessel

Dear Raghuram,

Please any code case or Interpretation.

Thanks & Regards

J.Gerald Jayakumar




On Sunday, 26 June, 2022 at 07:46:29 am GMT+4, Raghuram Bathula <raghurambathula@gmail.com> wrote:


Although no restriction in code preferable methoud could custom build modular furnace (with panel construction) at site

It is straight forward method for cir seams, however for long seams you have to work a methodology for placing coils locally using WRC 452 guidelines, probably  supplimented with an FEA to check thermal stresses

On Sat, Jun 25, 2022, 8:21 PM <pgoswami@rogers.com> wrote:

Hi,

It's allowed by Sec VIII, DIV1. Please see the highlighted clauses as below.

Thanks.

 

Pradip Goswami.P.Eng, IWE.

Independent Welding & Metallurgical Engineering Specialist

Saudi Aramco Approved Designated Project Welding Engineer (DPWR)

Qatar Petroleum Approved, SME-Materials & Corrosion Engineering.

Linkedin: https://www.linkedin.com/in/pradip-goswami-2999855/

Email:pgoswami@rogers.com,pradip.goswami@gmail.com

Cell/Whasapp:1-905-9793232

 

UW-40 PROCEDURES FOR POSTWELD HEAT TREATMENT:

From: vishal hirde <vishalhirde1988@gmail.com>
Sent: June 25, 2022 8:24 AM
To: materials-welding@googlegroups.com
Subject: PWHT Segment Wise for 9 Meter Dia Vessel

 

Dear All,

 

We are fabricating a Vessel of Diameter 9 Meter at Site, requires PWHT: Material Grade SA 516 Gr. 70.

 

 For Circumferential Joint PWHT can it be performed Segment Wise as diameter is more??

 

Pl. Confirm as per ASME Sec VIII Div 1 can it be done in Segment Wise. 

 

--

With Best Regards,

Vishal Hirde

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit
https://groups.google.com/d/msgid/materials-welding/CADxVubnGTyb%2BFpEFzdoU3gq%2BBVcYGERP65xWkWxr7QM_Q6EmkQ%40mail.gmail.com
.

Re: [MW:33177] RE: PWHT Segment Wise for 9 Meter Dia Vessel

Dear Raghuram,

Just for knowledge purpose. Do ASME Sec.VIII Div.I the applicable code permit LOCAL PWHT of Longitudinal seams.



Thanks & Regards

J.Gerald Jayakumar




On Sunday, 26 June, 2022 at 07:46:29 am GMT+4, Raghuram Bathula <raghurambathula@gmail.com> wrote:


Although no restriction in code preferable methoud could custom build modular furnace (with panel construction) at site

It is straight forward method for cir seams, however for long seams you have to work a methodology for placing coils locally using WRC 452 guidelines, probably  supplimented with an FEA to check thermal stresses

On Sat, Jun 25, 2022, 8:21 PM <pgoswami@rogers.com> wrote:

Hi,

It's allowed by Sec VIII, DIV1. Please see the highlighted clauses as below.

Thanks.

 

Pradip Goswami.P.Eng, IWE.

Independent Welding & Metallurgical Engineering Specialist

Saudi Aramco Approved Designated Project Welding Engineer (DPWR)

Qatar Petroleum Approved, SME-Materials & Corrosion Engineering.

Linkedin: https://www.linkedin.com/in/pradip-goswami-2999855/

Email:pgoswami@rogers.com,pradip.goswami@gmail.com

Cell/Whasapp:1-905-9793232

 

UW-40 PROCEDURES FOR POSTWELD HEAT TREATMENT:

From: vishal hirde <vishalhirde1988@gmail.com>
Sent: June 25, 2022 8:24 AM
To: materials-welding@googlegroups.com
Subject: PWHT Segment Wise for 9 Meter Dia Vessel

 

Dear All,

 

We are fabricating a Vessel of Diameter 9 Meter at Site, requires PWHT: Material Grade SA 516 Gr. 70.

 

 For Circumferential Joint PWHT can it be performed Segment Wise as diameter is more??

 

Pl. Confirm as per ASME Sec VIII Div 1 can it be done in Segment Wise. 

 

--

With Best Regards,

Vishal Hirde

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit
https://groups.google.com/d/msgid/materials-welding/CADxVubnGTyb%2BFpEFzdoU3gq%2BBVcYGERP65xWkWxr7QM_Q6EmkQ%40mail.gmail.com
.

Re: [MW:33176] RE: PWHT Segment Wise for 9 Meter Dia Vessel

Although no restriction in code preferable methoud could custom build modular furnace (with panel construction) at site

It is straight forward method for cir seams, however for long seams you have to work a methodology for placing coils locally using WRC 452 guidelines, probably  supplimented with an FEA to check thermal stresses

On Sat, Jun 25, 2022, 8:21 PM <pgoswami@rogers.com> wrote:

Hi,

It's allowed by Sec VIII, DIV1. Please see the highlighted clauses as below.

Thanks.

 

Pradip Goswami.P.Eng, IWE.

Independent Welding & Metallurgical Engineering Specialist

Saudi Aramco Approved Designated Project Welding Engineer (DPWR)

Qatar Petroleum Approved, SME-Materials & Corrosion Engineering.

Linkedin: https://www.linkedin.com/in/pradip-goswami-2999855/

Email:pgoswami@rogers.com,pradip.goswami@gmail.com

Cell/Whasapp:1-905-9793232

 

UW-40 PROCEDURES FOR POSTWELD HEAT TREATMENT:

From: vishal hirde <vishalhirde1988@gmail.com>
Sent: June 25, 2022 8:24 AM
To: materials-welding@googlegroups.com
Subject: PWHT Segment Wise for 9 Meter Dia Vessel

 

Dear All,

 

We are fabricating a Vessel of Diameter 9 Meter at Site, requires PWHT: Material Grade SA 516 Gr. 70.

 

 For Circumferential Joint PWHT can it be performed Segment Wise as diameter is more??

 

Pl. Confirm as per ASME Sec VIII Div 1 can it be done in Segment Wise. 

 

--

With Best Regards,

Vishal Hirde

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CADxVubnGTyb%2BFpEFzdoU3gq%2BBVcYGERP65xWkWxr7QM_Q6EmkQ%40mail.gmail.com.

Saturday, June 25, 2022

Re: [MW:33181] RE: PWHT Segment Wise for 9 Meter Dia Vessel

Dear Vishal 
As I understand  correctly , the vessel circumference is 9 mtr  and  your query is that you want to carry out the PWHT of the Circumferemtial seam in segments.

The answer is No . You have to carry out PWHT  of  ENTIRE Circumferencial joint in ONE cycle.
You can do it by LOCAL PWHT method by wrapping Electric Resitance Coil on job and attaching job thermocouples.

Many HT contracter are doing such type jobs regularly.
Thanks 
Vishwas Keskar 
IWE- International Welding Enginner

On Sat, 25 Jun 2022, 20:21 , <pgoswami@rogers.com> wrote:

Hi,

It's allowed by Sec VIII, DIV1. Please see the highlighted clauses as below.

Thanks.

 

Pradip Goswami.P.Eng, IWE.

Independent Welding & Metallurgical Engineering Specialist

Saudi Aramco Approved Designated Project Welding Engineer (DPWR)

Qatar Petroleum Approved, SME-Materials & Corrosion Engineering.

Linkedin: https://www.linkedin.com/in/pradip-goswami-2999855/

Email:pgoswami@rogers.com,pradip.goswami@gmail.com

Cell/Whasapp:1-905-9793232

 

UW-40 PROCEDURES FOR POSTWELD HEAT TREATMENT:

From: vishal hirde <vishalhirde1988@gmail.com>
Sent: June 25, 2022 8:24 AM
To: materials-welding@googlegroups.com
Subject: PWHT Segment Wise for 9 Meter Dia Vessel

 

Dear All,

 

We are fabricating a Vessel of Diameter 9 Meter at Site, requires PWHT: Material Grade SA 516 Gr. 70.

 

 For Circumferential Joint PWHT can it be performed Segment Wise as diameter is more??

 

Pl. Confirm as per ASME Sec VIII Div 1 can it be done in Segment Wise. 

 

--

With Best Regards,

Vishal Hirde




AVG logo

This email has been checked for viruses by AVG antivirus software.
www.avg.com


--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/!%26!AAAAAAAAAAAuAAAAAAAAABVPzeizzeRJsiPziIE5jXQBAMO2jhD3dRHOtM0AqgC7tuYAAAAAAA4AABAAAAD9ib%2BzVU4dRb/ePF01LBnGAQAAAAA%3D%40rogers.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CADder3Pk96%3DsLj8Qgn%2B17h7%2B5A3t7bYEJKFGBnBcm4b4kO7tRA%40mail.gmail.com.

Re: [MW:33177] RE: PWHT Segment Wise for 9 Meter Dia Vessel

What diameter can your furnace accommodate?. 9 Meter seems to be Big.

There are some options if your Furnace cannot accommodate.

1.  Try for a Temporary furnace with proper insulation and Heating arrangements. Hope there are some subcontractors available.
2. Try for LOCAL PWHT of the seams.
3. Below option may be useful if you have difficulty accommodating the Length in one Heat.

Thanks & Regards

J.Gerald Jayakumar




On Saturday, 25 June, 2022 at 06:57:06 pm GMT+4, pgoswami@rogers.com <pgoswami@rogers.com> wrote:


Hi,

It's allowed by Sec VIII, DIV1. Please see the highlighted clauses as below.

Thanks.

 

Pradip Goswami.P.Eng, IWE.

Independent Welding & Metallurgical Engineering Specialist

Saudi Aramco Approved Designated Project Welding Engineer (DPWR)

Qatar Petroleum Approved, SME-Materials & Corrosion Engineering.

Linkedin: https://www.linkedin.com/in/pradip-goswami-2999855/

Email:pgoswami@rogers.com,pradip.goswami@gmail.com

Cell/Whasapp:1-905-9793232

 

UW-40 PROCEDURES FOR POSTWELD HEAT TREATMENT:

From: vishal hirde <vishalhirde1988@gmail.com>
Sent: June 25, 2022 8:24 AM
To: materials-welding@googlegroups.com
Subject: PWHT Segment Wise for 9 Meter Dia Vessel

 

Dear All,

 

We are fabricating a Vessel of Diameter 9 Meter at Site, requires PWHT: Material Grade SA 516 Gr. 70.

 

 For Circumferential Joint PWHT can it be performed Segment Wise as diameter is more??

 

Pl. Confirm as per ASME Sec VIII Div 1 can it be done in Segment Wise. 

 

--

With Best Regards,

Vishal Hirde




AVG logo

This email has been checked for viruses by AVG antivirus software.
www.avg.com


--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/!%26!AAAAAAAAAAAuAAAAAAAAABVPzeizzeRJsiPziIE5jXQBAMO2jhD3dRHOtM0AqgC7tuYAAAAAAA4AABAAAAD9ib%2BzVU4dRb/ePF01LBnGAQAAAAA%3D%40rogers.com.

[MW:33175] RE: PWHT Segment Wise for 9 Meter Dia Vessel

Hi,

It's allowed by Sec VIII, DIV1. Please see the highlighted clauses as below.

Thanks.

 

Pradip Goswami.P.Eng, IWE.

Independent Welding & Metallurgical Engineering Specialist

Saudi Aramco Approved Designated Project Welding Engineer (DPWR)

Qatar Petroleum Approved, SME-Materials & Corrosion Engineering.

Linkedin: https://www.linkedin.com/in/pradip-goswami-2999855/

Email:pgoswami@rogers.com,pradip.goswami@gmail.com

Cell/Whasapp:1-905-9793232

 

UW-40 PROCEDURES FOR POSTWELD HEAT TREATMENT:

From: vishal hirde <vishalhirde1988@gmail.com>
Sent: June 25, 2022 8:24 AM
To: materials-welding@googlegroups.com
Subject: PWHT Segment Wise for 9 Meter Dia Vessel

 

Dear All,

 

We are fabricating a Vessel of Diameter 9 Meter at Site, requires PWHT: Material Grade SA 516 Gr. 70.

 

 For Circumferential Joint PWHT can it be performed Segment Wise as diameter is more??

 

Pl. Confirm as per ASME Sec VIII Div 1 can it be done in Segment Wise. 

 

--

With Best Regards,

Vishal Hirde




AVG logo

This email has been checked for viruses by AVG antivirus software.
www.avg.com


Friday, June 24, 2022

[MW:33175] Consumable insert (QW 404.22) vs preplaced fillermetal (QW 404.58)

What is difference between Consumable insert (QW 404.22) and preplaced fillermetal (QW 404.58) in ASME BPVC Sec IX?
Consumable inserts that conform to SFA-5.30 (ASME BPVC IIC), where as no such refrence or difinition for preplaced fillermetal.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/aa6754a6-c2c8-4aa7-ab0d-cfa77efa4905n%40googlegroups.com.

Monday, June 20, 2022

[MW:33165] Acceptance of Excess weld/ hump/ protrution in Weld overlay

Gents,

Could you please advise the acceptance criteria for excess weld / circumferential hump / protrusion in weld overlay of API5LD weld overlay pipes?
Visual inspection criteria addresses under thickness of 0.8 mm only. it does not say about circumferential humps acceptance limit.


Thanks & Regards
Muhammed Ibrahim PK

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CALOPgmNCWcKP-OBPEEsbiuTRq0GObbuOJxiiipVt3XAO6rZYcQ%40mail.gmail.com.

Re: [MW:33162] PQR test required

RT is not mandatory according to ASME sec IX. 

1. It is to help you for destructive testing sampling you can discard the defective location.
2. Most of the customer expects RT examination
3. Additionally you have an provision to prefer UT in lieu of RT

On Mon, 20 Jun 2022 at 12:11, Manoj Singh <manoj.singh1178@gmail.com> wrote:
Hi Teams,

want to know while qualifying PQR is RT is mandatory if use pls. give reference.



Regards 

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAPkJdRLq5NgcUuh8B6c-s7C7iJCs36LvizYGMY%3Dmx_u%2BiAF8jA%40mail.gmail.com.
--
Regards
Ramesh Babu Balaram
Head QA/QC
Zetwerk Manufacturing Businesses Private Limited
Mobile: +91 98 4 053 13 55

>>>DONATE NOW<<<
SUPPORT ZETWERK'S CAMPAIGN TO FEED THE VURNERABLE MIGRANT FACTORY WORKER POPULATION.
Contribute generously. Each donation will go towards essential ration kits.
Let's come together as a nation so that they don't have to go hungry

This information may be confidential and/or privileged. Use of this information by anyone other than the intended recipient is prohibited. If you receive this in error, please inform the sender and remove any record of this message

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAHJfB2k%2BVGDHrJwvCMQ8mNt%3DFAik6Ksa3XkJ%2BvxMZmy%3Drf4DMg%40mail.gmail.com.

Saturday, June 18, 2022

Re: [MW:33160] TEST REQUIRED

Generally while qualifying PQR following shall report

Tension
Bend 
hardness (additional)
Macro (additional)

According to project spec
Toughness test 
Hardness 
Macro 

On Sat, 18 Jun 2022 at 15:04, Kannayeram Gnanapandithan <kgpandithan@gmail.com> wrote:
Hardness test requirements, is it required as per code or Project specification requirements

THANKS & BEST REGARDS,
KG.PANDITHAN, BE, IWE,  CSWIP 3.1,
ISO 9712 Level 2 in VT,
ASNT-Level II in PT,MT,RT & UT,
LA ISO 9001-2015,
International Welding Engineer. 
CONSULTANT-WELDING & QUALITY
Mobile no: +919940739349


On Fri, Jun 17, 2022 at 7:53 PM Rameshbabu B <rameshbabu.b@zetwerk.com> wrote:
Hi Sujit, 

Referring to QW-451.1 the following tests shall be conducted.

2 Transverse tensile
2 Root Bend
2 Face bend

Additionally, you can advise the laboratory to perform a hardness test for Base, Weld, and HAZ which is common when qualifying a PQR


On Fri, Jun 17, 2022 at 6:03 PM sujit kumar <sujitkumar19942@gmail.com> wrote:
Hii Experts,

hope all is well.

I want to know which test is required for WPS and how many tests are required as per ASME section IX.?

PLATE SPECIFICATION-SA516  GR70
PLATE THICKNESS-10MM
FILLER USED-ER-70S2
ELECTRODE USED-E-7018
 TOUGHNESS TEST NOT REQUIRED



Best regards
Sujit Kumar

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/0d00b35e-1d18-400f-9bf6-a9a55001f9a0n%40googlegroups.com.


--

Ramesh Babu Balaram

Corporate Head, Quality

The Oriental Towers, No. 461, 1st Floor, 17th Cross Road, 4th Sector,

Sector 4, HSR Layout, Bengaluru, Karnataka 560102.

M 9840531355  E rameshbabu.b@zetwerk.com  W zetwerk.com

App Green Footer Image Please consider your environmental responsibility. Before printing this e-mail message, ask yourself whether you really need a hard copy.



This information may be confidential and/or privileged. Use of this information by anyone other than the intended recipient is prohibited. If you receive this in error, please inform the sender and remove any record of this message

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAHJfB2mOnqEbUYXM%2Bt4jZ9hgrOGD-nObkLesQ1%2BGgmyTDZWgAA%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAJzm4eOE2QFhk%2BtDZn-BWDerVf86PbJsXZmAp3sBgESBWyB-3Q%40mail.gmail.com.
--
Regards
Ramesh Babu Balaram
Head QA/QC
Zetwerk Manufacturing Businesses Private Limited
Mobile: +91 98 4 053 13 55

>>>DONATE NOW<<<
SUPPORT ZETWERK'S CAMPAIGN TO FEED THE VURNERABLE MIGRANT FACTORY WORKER POPULATION.
Contribute generously. Each donation will go towards essential ration kits.
Let's come together as a nation so that they don't have to go hungry

This information may be confidential and/or privileged. Use of this information by anyone other than the intended recipient is prohibited. If you receive this in error, please inform the sender and remove any record of this message

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAHJfB2mv9LLaBc-XM-6%3DmLkY%3DGF6e4Wj8kdJiHrH996V5DBgVw%40mail.gmail.com.

[MW:35738] ASME IX WPS Qualification Query: GTAW + FCAW with Multiple PQRs

Dear Welding Experts, I'm currently preparing a Welding Procedure Specification (WPS) and have encountered a request to qualify a GTAW +...