Thursday, February 16, 2012

Re: [MW:13711] IQI Selection

 Dear Mr.Sivakumar,
 
For ensitivity calculation you can consider reinofrcement as per sec v.The reinforcement means not only face reinforcement, that is inclusion of root also.so u can consider the both.If u consider the both you may get better sensitivity value closed to your requirement.
 
But as per  EN code , you shall only consider the base metal thickness.

On Thu, Feb 16, 2012 at 9:12 AM, S.Sundar Rajan <as_sundarrajan@yahoo.com> wrote:
Dear Mr.siva kumar,

Internal protrusion or root penetration need not be considered while choosing IQI. The thickness of the base metal and reinforcement should be added. Because the width of the internal protrusion is very narrow usually (2 to 3 mm) . Only the reinforcement is covering full width of the bevel preparation.
 
With Regards,
s.sundarrajan,
QA/QC Inspector,
Special technical services LLC, Muscat,
M: +96898217243.


From: Siva Kumar <mailmrsiva@yahoo.com>
To: "materials-welding@googlegroups.com" <materials-welding@googlegroups.com>
Sent: Wednesday, 15 February 2012 4:47 PM
Subject: [MW:13705] IQI Selection

Dear All,
 
As per ASME SEC-V, ART -2,T-276.2, for IQI selection, it has been mentioned that the weld reinforcement as per the referencing code can be added with nominal wall thickness of the pipe.
 
As per B31.3, the acceptance for weld reinforcement or internal protrusion for wall thickness above 6mm to 13mm is 3mm.
 
If we take a 4" sch std pipe, thickness of which is 6.02mm, Can we take into consideration 6.02mm + 3mm for reinforcement + 3mm for internal protrusion - total 12.02mm as nominal wall thickness for the essential wire to be visible as per Table T276 in Sec V art 2?
 
If so, is there any reference that internal protrusion can also be considered?
 
Please suggest.
 
Siva.
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.


--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.



--

With Regards,

 

Muthukumaran P

Asst. Manager(Qa/Qc) / L&T - HCP (I)

HRS Pipeline Project / Abudhabi

Ph:+971503297345


--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:35738] ASME IX WPS Qualification Query: GTAW + FCAW with Multiple PQRs

Dear Welding Experts, I'm currently preparing a Welding Procedure Specification (WPS) and have encountered a request to qualify a GTAW +...