Hello Asad Azmi,

What was the method used for preheating?

The soot formation as seen on the photos attached should not have any adverse effect on the material, however you will need to clean it before further processing.

Regards

George V Aliyattukudy

vijigeorge@dugas.ae

P Please consider the environment before printing this e-mail.

 

From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of asad azmi
Sent: 27 February 2012 17:59
To: materials-welding@googlegroups.com
Subject: [MW:13789] effect of SOOT formation on base material

 

Dear All,

 

Greetings.

 

During preheating of a weld joint  SOOT( Black spots) was observed on the base material ( SA 516 GR 70- 50 Thk). Please refer attached photo.

 

Please explain is there any  adverse effect on base material becuase  of the SOOT formation.

 

Thanks & Regards

 

Asad Azmi

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:35737] Bend Test and Tensile Test failed for ET45 Micro Welded Coupon

Hi As its %elongation is very low  Better try buttering on jt surrace with ductile consumable like pure Ni i. E Ni1 And later weld jt with c...