QW-405.2
A change from any position to the vertical
position uphill progression. Vertical-uphill progression
(e.g., 3G, 5G, or 6G position) qualifies for all positions.
In uphill progression, a change from stringer bead to weave
bead. This variable does not apply when a WPS is qualified
with a PWHT above the upper transformation temperature
or when an austenitic material is solution annealed after
welding.
On Mon, Jun 20, 2011 at 2:37 PM, K.Babu <kbabupsg@gmail.com> wrote:
HiAs per Cl. QW 405.2 , in WPS qualification, Vertical Up position qualifies all position.But always, the class people not ready to accept this ?Is there any Official interpretation or clarification given by ASME or AWS on this.
On Sun, Jun 19, 2011 at 10:22 PM, Dinesh Somwanshi <som.din@gmail.com> wrote:
CAN YOU EXPLAIN BRIEF--
On Sat, Jun 18, 2011 at 6:12 PM, K.Babu <kbabupsg@gmail.com> wrote:--Gents,Any one have the official interpretation for the above, as per ASME sec IX or AWS D1.1 for WPS qualification
--
Thanks & regards,
K.Babu
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
--
Thanks & regards,
K.Babu
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
No comments:
Post a Comment