what is the manufacturing standard for these elbows?

On Thu, Jun 9, 2011 at 4:28 PM, Sampath Kumar <skthatham@gmail.com> wrote:
Dear Experts,
 
I would like to know the tolerance level of ovaltiy in elbows of size 84" and as well pls tell me in which code and standard it says so.What is the solution if we have ovaltiy of 54mm,56mm and 66mm all in different elbows.All SSelbows.
Regards
Sampath


--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:35289] Welding consumable for S355J2WP material

S355 J2 WP  is a weathering structural steel  It has better atmospheric corrosion resistance. Use E 8018 - W1/W2  Electrodes This is regular...