Re: [MW:11270] RE: 11202] Welding consumable for CD3Mn

Dear

As your Below mail Material is O.K as per code requirement. you are right.




Kind Regards,

Vijay Malusare.
(Sr. QA/QC Engineer.)

On Mon, Jun 6, 2011 at 4:31 PM, vikas shelke <vikas.shelke84@gmail.com> wrote:
Dear All,
     In a vessel we used SA 516 Gr. 70 Plate for Dished ends (12 Thk).
Chemical Analysis (Lab Tested) of Plate (values) observed are,
 
 Chromium          (0.018       Req. 0.34 max) ,
 Nickel                 (0.021       Req. 0.43 max),
 Molybdenum      (0.008       Req. 0.13 max),
 Copper               (0.013       Req. 0.43 max).
 Vanadium          ( Nil
 Niobium              ( Nil
 Titanium             ( Nil
 
     Our customer is not accepting the material Since the above elements are much lesser than the specified.
We explained 1) since as per spec.only maximum values are specified it is acceptable.
                     2)  CE is within limit.
           But he is not accepting the same.
 
What to do ? Please, help me.
 
 
Regards,
 
Vikas.
         

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.



-


--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:35289] Welding consumable for S355J2WP material

S355 J2 WP  is a weathering structural steel  It has better atmospheric corrosion resistance. Use E 8018 - W1/W2  Electrodes This is regular...