Thursday, June 2, 2011

[MW:11244] possibility of skip WQT based on other WQTs

Hi,

I have 3 WPS based on AWS B2.1, Process GTAW.
  1. WPS-002 (M43 to M8) – Filler Metal ER 308L (F6)
  2. WPS-004 (M43 to unassigned Ni263) - Filler Metal B21B783  and
  3. WPS-005 (M8 to M8) – Filler Metal ER 308L (F6)
I would like to carry out WQT on our welders. I have been informed that I can skip WQT on WPS-002 (item 1 above) if a welder is successful on WPS-004 & WPS-005 (item 2 & 3 above). Is this true?

Any explanation and reference to the code? I would appreciate it.

Thank you.
Azril

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:35289] Welding consumable for S355J2WP material

S355 J2 WP  is a weathering structural steel  It has better atmospheric corrosion resistance. Use E 8018 - W1/W2  Electrodes This is regular...