Friday, February 18, 2011

RE: [MW:9928] Corten & carbon Steel weldability

There is no SA-242 –The S indicates that the material is included in ASME Section II and has ASME Code allowable stresses in Sc II Part D.  ASTM A-242 is not included in QW-422 and therefore is an “Unassigned Metal” per ASME Section IX (See QW-424) and does not have a P-No.  Because it is unassigned all welds must be separately qualified:  i.e. unassigned to unassigned, unassigned to P-No 1, unassigned to P-No 2, etc.

 

From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of Pradeep Sawant
Sent: Thursday, February 17, 2011 11:23 PM
To: materials-welding@googlegroups.com
Subject: Re: [MW:9919] Corten & carbon Steel weldability

 

Dear,

P no 1 and equivalent SA 242 for welding choose SFA 5.29 W cu content wire In FCAW.(E81T1W2)

Regards
Pradeep

 


From: Zakaria ghrab <zakaria.ghrab@gmail.com>
To: materials-welding@googlegroups.com
Sent: Thu, 17 February, 2011 9:14:27 PM
Subject: [MW:9916] Corten & carbon Steel weldability


Hi all,

  I need to know the P number of corten steels, i have on PQR according ASME sect IX corten to corten, i need to use it to prepare WPS for Carbon steels but i have doute Corten is PN°1 or PN°3, serashing in internet : Equivalent Corten is ASTM SA 242, is it true?
--
GHRAB Zakaria

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:35289] Welding consumable for S355J2WP material

S355 J2 WP  is a weathering structural steel  It has better atmospheric corrosion resistance. Use E 8018 - W1/W2  Electrodes This is regular...