Dear Sir,
Many thanks for your information.
For SMAW, have selected the same but for GTAW we are using ER 70S2. Is it right?
Also request you to inform from where I can select the same, as have gone through the ASME sec 2 Part c but not able to succeed.
Thanks.
Regards,
Abhay
Ext 448
M +91 9898031162
IMPORTANT NOTICE:
This email may be confidential, may be legally privileged, and is for the intended recipient only. Unauthorized access, disclosure, copying, distribution, or reliance on any of it by anyone else is prohibited and may be a criminal offense. Please delete if obtained in error and email confirmation to the sender.
From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of james gerald
Sent: Monday, February 14, 2011 10:47 AM
To: materials-welding@googlegroups.com
Subject: Re: [MW:9861] electrode selection of WPS of SA 333 Gr 6 low temp piping, GTAW +SMAW
GTAW - ER80SNi1 SMAW - E7018-1 The above can be used to weld A333 Gr.6 Pipe upto MDMT of -45degC J.GERALD JAYAKUMAR 00919344954677
Dear Sirs, Pl advise how can select the electrodes for SA 333 Gr 6 (P1 and G1) low temp pipe. I want to prepare WPS / PQR and then also WPQ for our current project. Have selected the thickness around 5.55 mm (2 “S 80 pipe) for preparing WPS. We followed the process of root run by GTAW and then by SMAW. Regards, Abhay Ext 448 IMPORTANT NOTICE: -- |
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
No comments:
Post a Comment