Re: [MW:9861] electrode selection of WPS of SA 333 Gr 6 low temp piping, GTAW +SMAW

GTAW - ER80SNi1
SMAW - E7018-1
 
The above can be used to weld A333 Gr.6 Pipe upto MDMT of -45degC

J.GERALD JAYAKUMAR
00919344954677
 


--- On Mon, 2/14/11, Abhonkar, Abhay (NAR) <AAbhonkar@Dresser-Rand.com> wrote:

From: Abhonkar, Abhay (NAR) <AAbhonkar@Dresser-Rand.com>
Subject: [MW:9855] electrode selection of WPS of SA 333 Gr 6 low temp piping, GTAW +SMAW
To: materials-welding@googlegroups.com
Date: Monday, February 14, 2011, 3:57 AM

Dear Sirs,

Pl advise how can select the electrodes for SA 333 Gr 6 (P1 and G1) low temp pipe.

I want to prepare WPS / PQR and then also WPQ for our current project.

Have selected the thickness around 5.55 mm (2 "S 80 pipe) for preparing WPS.

 

We followed the process of root run by GTAW and then by SMAW.

 

Regards,

Abhay

Ext 448

 

IMPORTANT NOTICE:
This email may be confidential, may be legally privileged, and is for the intended recipient only. Unauthorized access, disclosure, copying, distribution, or reliance on any of it by anyone else is prohibited and may be a criminal offense. Please delete if obtained in error and email confirmation to the sender.


--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34920] Tubesheet Hole step

Hello Team, I have one question any tolerance given for tubesheet Hole step. Please do needful. Regards, AP  -- https://materials-...