Re: [MW:9860] Electrode Make Clarification

Dear friend

As per  ASME sec IX   Electrode Brand name is Not essential variable ,   you can use welder comfortable any  electrode   Since u r using low Hydrogen coated electrode DRY them in oven for min room temp 1hour  and use .even Adour  make will give user friendly  as i am comfortable with


Regards
RAVIKUMAR T S




From:        prabhu duraisamy <prabu.mptmt@gmail.com>
To:        <materials-welding@googlegroups.com>
Date:        02/13/2011 10:19 AM
Subject:        [MW:9851] Electrode Make Clarification
Sent by:        <materials-welding@googlegroups.com>




Dear Friends,
                    As per our approved WPS says welding electrode 6010 & 7018 make is ESAB, but our welders is not comfortable for ESAB 6010, They confortable to weld Lincoln Make. please advice me it is allow to weld Lincoln Make. if code is saying anything please give the details.

--

Thanks and Regards
 
Prabhu Duraisamy
QA/QC Engineer
Internal Auditor [ISO 9001, 14001 & OSHAS 18001]
________________________________________
Abu Dhabi, UAE
M.UAE: +971-501341046
M.INDIA: +91-9942281543
E: prabu_preyan@yahoo.co.in
E: prabu.mptmt@gmail.com

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at
http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34920] Tubesheet Hole step

Hello Team, I have one question any tolerance given for tubesheet Hole step. Please do needful. Regards, AP  -- https://materials-...