RE: [MW:9859] importance of Nitrogen in analysis of SS 304L

“N” is specified element and required to be reported on MTC for SA 240 TP 304 L

 

From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of Welding Material
Sent: Monday, February 14, 2011 10:11 AM
To: materials-welding@googlegroups.com
Subject: [MW:9856] importance of Nitrogen in analysis of SS 304L

 

Dear All,

 

Anybody can tell me that how nitrogen Analysis is important while analysising chemical composition of SS 304 L Plate.

In Lab test report Except Nitrogen all elements are within range as per SA 240 TP 304 L ; but Nitrogen is not checked.

 