Wednesday, February 2, 2011

Re: [MW:9661] Distortion Control in SS welding

In addition to below you can provide chiling effect from inside if there is access.
Chiling effect means spraying of water from inside adjacent to the weld joint.
 
regards
Gurmeet SIngh

On Sat, Jan 29, 2011 at 8:51 AM, yusufkhan pathan <yusufkhanp97@gmail.com> wrote:
Dear All,
 
Please suggest me any information related to distortion control in Stainless Steel welding. usually while welding lower thickness (bet 4 to 8 mm).
 
Thanks in advance.
 
Regards.
Yusufkhan.Pathan
8008804165

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:35289] Welding consumable for S355J2WP material

S355 J2 WP  is a weathering structural steel  It has better atmospheric corrosion resistance. Use E 8018 - W1/W2  Electrodes This is regular...