Re: [MW:9644] RE: preparation WPS & PQR

Hi

Please read and understand the suggested format given in ASME Sec IX:
QW-482 for WPS
QW-483 for PQR

Self help is the best help !

Regards

Prem Nautiyal

On Tue, 01 Feb 2011 13:47:59 +0530 wrote
>Dear experts, Could you please give some guidelines or codes, references on how to prepare WPS & PQR? I'm sure your valuable inputs will help me to prepare this.Thank you,Ilan **********************************************************************Borouge is a leading provider of value creating, innovative plastics solutions for customers in the Middle East, Asia-Pacific and Africa. Borouge employs unique Borstar® technology to produce differentiated products for high-value infrastructure applications, including water, gas and industrial pipe systems, power and communication cables, advanced packaging and automotive components. Borouge's state-of-the-art petrochemical complex is located at Ruwais, Abu Dhabi in the United Arab Emirates. ===================================================================================
>CONFIDENTIALITY NOTICEThis email and any files transmitted with it are confidential and intended solely for the use of the individual or entity to whom they are addressed. If you have received this email in error please delete the email and any attachment(s) and notify the sender.This footnote also confirms that this email message has been scanned for the presence of computer viruses.
>============================================================================================================= 




--
>
To post to this group, send email to materials-welding@googlegroups.com
>
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
>
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
>
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
>


PREM S NAUTIYAL
CELL : 9769316004

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:35289] Welding consumable for S355J2WP material

S355 J2 WP  is a weathering structural steel  It has better atmospheric corrosion resistance. Use E 8018 - W1/W2  Electrodes This is regular...