Friday, February 18, 2011

[MW:9920] Temperbead welding

Gents,
ASME SEC IX QW290 permits temperbead welding as an alternative method
to avoid heat traetment. I have few pipe joints which are internally
coated(sleeved internally to protect the weld area) and thk>20mm.
Material is A106 Gr-B and design pressure 3500 psig.Welding will be
downhand, by using E6010+7010)

Can I Qualify temper bead procedure and apply it??


Expert advise will be appreciated.


Thanks
Shaji


--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:35289] Welding consumable for S355J2WP material

S355 J2 WP  is a weathering structural steel  It has better atmospheric corrosion resistance. Use E 8018 - W1/W2  Electrodes This is regular...