You can use filler :- ErNiCrMo6 and process GTAW.
With kind regards,
Vinod Kumar Kataria
GM - Operations
Bliss Anand Private Limited,
92B/93B Sector 5
IMT Manesar,Gurgaon,
National Capital Region Delhi.
India .
Phone : +91-124-4366000 (9 Lines)
Mobile Phone : +91-9560199004
Fax : +91-124-2290884
From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of praveen nair
Sent: Tuesday, February 01, 2011 2:22 PM
To: materials-welding@googlegroups.com
Subject: [MW:9632] welding of inconel 600
dear experts, |
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
No comments:
Post a Comment