CAD welding is named after Dr Cadwell. It is a form of thermite welding used
to bond wire to metal, typically used in the rail industry.

With kind regards,
Vinod Kumar Kataria
GM - Operations
Bliss Anand Private Limited,
92B/93B Sector 5
IMT Manesar,Gurgaon,
National Capital Region Delhi.
India .
Phone : +91-124-4366000 (9 Lines)
Mobile Phone : +91-9560199004
Fax : +91-124-2290884

-----Original Message-----
From: materials-welding@googlegroups.com
[mailto:materials-welding@googlegroups.com] On Behalf Of Nixon Joseph
Sent: Tuesday, February 01, 2011 12:03 PM
To: materials-welding@googlegroups.com
Subject: [MW:9622] RE: 9621] CAD WELD

Hi

What IS MEAN BY cad welding?

Regards

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to
materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at
http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and
meant for educational purposes only, Users must take their own decisions
w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:35289] Welding consumable for S355J2WP material