RE: [MW:8876] ELECTRODE - Change in AWS classification for weld overlay

Yes.I accept.

Thanks & Regards,

(Karthik)

Karthikeyan.S
QA/QC Manager
Getabec Energy Co.,Ltd.
379,Moo6,Soi8,Nikhomphatana,
Rayong-21180,
Thailand.
Phone: 0066 38 897035-8 (Off)
Fax: 0066 38 897034
Hand Phone: 0066 892512282


--- On Wed, 12/22/10, Bathula Raghuram (Mumbai - PIPING) <R.Bathula@ticb.com> wrote:

From: Bathula Raghuram (Mumbai - PIPING) <R.Bathula@ticb.com>
Subject: RE: [MW:8874] ELECTRODE - Change in AWS classification for weld overlay
To: "'materials-welding@googlegroups.com'" <materials-welding@googlegroups.com>
Date: Wednesday, December 22, 2010, 12:40 PM

Please read carefully QW404.37, in case of weld overlay AWS classification will be an essential variable

 

From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of Karthik
Sent: Wednesday, December 22, 2010 10:58 AM
To: materials-welding@googlegroups.com
Subject: RE: [MW:8872] ELECTRODE - Change in AWS classification for weld overlay

 

E309-L and E316L are both same F number(5) and A number (8),SFA number 5.4. So it is acceptable.

Thanks & Regards,

 

(Karthik)

 


--- On Wed, 12/22/10, Bathula Raghuram (Mumbai - PIPING) <R.Bathula@ticb.com> wrote:


From: Bathula Raghuram (Mumbai - PIPING) <R.Bathula@ticb.com>
Subject: RE: [MW:8868] ELECTRODE - Change in AWS classification for weld overlay
To: "'materials-welding@googlegroups.com'" <materials-welding@googlegroups.com>
Date: Wednesday, December 22, 2010, 12:09 PM

Each AWS classification of A-No. 8 analysis of table QW-442, shall require separate WPS qualification (QW404.37).

-----Original Message-----
From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of KUMAR
Sent: Wednesday, December 22, 2010 10:26 AM
To: materials-welding@googlegroups.com
Subject: [MW:8866] ELECTRODE

Dear sir,

In weldoverlay  smaw  process welding, the changing electrode E309L in
place of E316L is acceptableor not?  It  mentioned in WPS that E309L
is for barrier Layer and E316L for clad layer

Thanks and regards
M.Kumar





 


--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34919] Welder qualification certificate

Dear All     anyone can share a format for welder certificate and card format        Thanks & Best Regards Saleem manhappulath Mob:+9665...