Re: [MW:8870] WPQT P.No & F.No. Range

Dear Limesh,
 
Absolutely yes for both your questions as per ASME Sec.IX 2010.
 
But you also need to look into the practical application when applying this wide range.
 
Regards,
 
Praveen Alavandar
Sr.Welding Engineer
Muscat
 


--- On Wed, 12/22/10, limesh M <limesh78@gmail.com> wrote:

From: limesh M <limesh78@gmail.com>
Subject: [MW:0] WPQT P.No & F.No. Range
To: "Materials & Welding" <materials-welding@googlegroups.com>
Date: Wednesday, December 22, 2010, 10:26 AM

Dear All,

Welding Code: ASME BPVC SEC IX, 2010 edition

 
A welder qualified on P No.45 material by using F No. 43 filler wire. I need clarification on following queries based on QW 423.1 and QW 433.
 
1. Is the welder qualified to weld P.No. 34, 41, 42, 43, 44, 45, 46, 47, 48 and 49 materials?
 

2. Is the welder qualified to use F.No. 34, 41, 42, 43, 44, 45 and 46 consumables?

 

 

Regards,

 

Limesh

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34920] Tubesheet Hole step

Hello Team, I have one question any tolerance given for tubesheet Hole step. Please do needful. Regards, AP  -- https://materials-...