Hi Asad

ASME sec VIII Div 1 - gives guidance for fabrication heat treatment.

But, for accepting materials you have to review the TC with respect to
ASME II , Part A, as per the requirement of SA 387 GR 12 CL2 The
heat treatment soaking time in TC to meet this spec and the
corresponding general spec in ASME Sec II, part A.

Thanks

Murugesan

On 12/11/10, asad azmi <azmiasadayub@gmail.com> wrote:
> Dear All,
>
> Greetings.
>
> for a vessel to be fabricated as per ASME SEC VIII DIV 1.
>
> Shell material - SA 387 GR 12 CL2 80 THK,
>
> AS PER UCS 56 Soaking time for PWHT for this thickness is 195 minutes.
> vessel required simulation cycles( 3 cycles) PWHT.
>
> AS per the test certificates the heat treatment simulation cycles for test
> coupon was done for 504 minutes only.
>
>
> *Pls inform me whether the Test certificate/results can be accepted as the
> soaking hours are less than the requirement.*
>
>
> Regards
>
> Asad Azmi
>
> --
> To post to this group, send email to materials-welding@googlegroups.com
> To unsubscribe from this group, send email to
> materials-welding+unsubscribe@googlegroups.com
> For more options, visit this group's bolg at
> http://materials-welding.blogspot.com/
> The views expressed/exchnaged in this group are members personel views and
> meant for educational purposes only, Users must take their own decisions
> w.r.t. applicable code/standard/contract documents.
>

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34919] Welder qualification certificate

Dear All     anyone can share a format for welder certificate and card format        Thanks & Best Regards Saleem manhappulath Mob:+9665...