Dear Asad,
               One set of charpy is fine. Either longitudinal or tranverse orientation.

2010/12/11 asad azmi <azmiasadayub@gmail.com>
Dear All,
 
Greetings.
 
for a vessel to be fabricated as per ASME SEC VIII DIV 1.
 
Shell Plate material  -  SA  387 GR 12 CL2   80 THK,
 
pls inform me how many minimun test specimens are required for  IMPACT Testing for test coupon.
 
 
Regards
 
Asad Azmi

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.



--
regards,
Harish.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34919] Welder qualification certificate

Dear All     anyone can share a format for welder certificate and card format        Thanks & Best Regards Saleem manhappulath Mob:+9665...