Hi,
You can do Immediete post heat and finish the weld after some days with preheat again.
No neeed to cut.you can do preheat again and start welding.

Thanks & Regards,

(Karthik)

Karthikeyan.S
QA/QC Manager
Getabec Energy Co.,Ltd.
379,Moo6,Soi8,Nikhomphatana,
Rayong-21180,
Thailand.
Phone: 0066 38 897035-8 (Off)
Fax: 0066 38 897034
Hand Phone: 0066 892512282


--- On Fri, 12/10/10, srinivas rao <ksrvasu@gmail.com> wrote:

From: srinivas rao <ksrvasu@gmail.com>
Subject: [MW:8670] Alloy Steel
To: materials-welding@googlegroups.com
Date: Friday, December 10, 2010, 10:24 PM

Dear All,

While welding of  ASTM A335 Gr P11, what to do if welding was stopped after Root Pass ,Hot Pass and One Fill-Up done without completing the job? Can we do immediately Post Heating for the un-finished job and continue welding next day? or Should we cut and re-weld the joint?

I have one more doubt... In the above situation what if welding and Pre-heating(coil heating)  was stopped due to power failure for 2 to 3 hrs and the joint has to come to room temp. Should the joint be cut and re-welded?

Regards,

Vasu


--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34920] Tubesheet Hole step

Hello Team, I have one question any tolerance given for tubesheet Hole step. Please do needful. Regards, AP  -- https://materials-...