Re: [MW:8633] Electrode Qualification Test

You can not have thickmess of 13mm for Electrode qualification of ER70S-6.
 
Refer SFA 5.18 Fig 1 (Page no. 408 of 2007 ASME Sec II C) for details of requirements. It will also give the answers of your other doubts.
 
 
Jaydeep Joshi

On Thu, Dec 9, 2010 at 3:47 PM, Pushpraj Anand <pushprajanand34@gmail.com> wrote:
Dear all,
 
We want Electrode Qualification Test on Filler wire for MIG ER70S-6 AWS SFA number-5.18
 
Kindly suggest me- what is root gap between & what is the backing plate thickness for 12mm thickness plate.
 


--
Regards,
Pushpraj Anand

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34920] Tubesheet Hole step

Hello Team, I have one question any tolerance given for tubesheet Hole step. Please do needful. Regards, AP  -- https://materials-...