Wednesday, December 8, 2010

Re: [MW:8581] heating and cooling rate for the heat treatment

Hi marcelo,
 
You can refer Table 331.1.1 Requirement for heat tratment in ASME B 31.3, Page 67 in 2008 Edition)
 
Regards,
 
Subramanian Esakkimuthu.

On Wed, Dec 1, 2010 at 1:01 PM, Shiv Dutt Mishra Mishra <gopu301182@gmail.com> wrote:
please check on following details.
ASME SECIII Div-1
1.PWHT & PROCEDURE: UW-10/40
2.REQUIREMENT OF PWHT- UCS-56
3.H.T. & MATL TEST COUPON-UCS-85
4.PWHT NF/HA/CL:UNF-56/UHA-32/UCL-34
5.H.T. AUSTE. CR-NI STEEL: UHA-105(NM)

SDM

On 12/1/10, marcelo soares ribeiro <marceloinspetorn1@gmail.com> wrote:
> RIO DE JANEIRO, 1st DECEMBER
>
> dear sirs
>
> can anyone suggest where meet   heating and cooling rate for the heat
> treatment in code ansi/asme B31.3?
>
> best regards
>
> marcelo s. ribeiro
> welding inspector-level 1
>
> --
> To post to this group, send email to materials-welding@googlegroups.com
> To unsubscribe from this group, send email to
> materials-welding+unsubscribe@googlegroups.com
> For more options, visit this group's bolg at
> http://materials-welding.blogspot.com/
> The views expressed/exchnaged in this group are members personel views and
> meant for educational purposes only, Users must take their own decisions
> w.r.t. applicable code/standard/contract documents.
>


--
Thanks,
S.D.Mishra
Mob- 09589444897 (M.P./C.G.)
        09766916581 (Maharastra)

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.



--

Regards,

E.Subramanian


--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34919] Welder qualification certificate

Dear All     anyone can share a format for welder certificate and card format        Thanks & Best Regards Saleem manhappulath Mob:+9665...