Re: [MW:8562] phased array vs. RT

Our experience is: phased array is much better than RT. RT could not clearly reveal the mico crack in the fir-tree design of turbine blades. But with phased array, we could get all the quantitative details (length, breadth, depth) accurately and could image the micro-crack also clearly.
All the best,
best regards,
Vaidehi.
----------------------------------------------------------------------------------------------------------
IGCAR, Kalpakkam.
====================================
----- Original Message -----
Sent: Tue, Dec 07, 10 1:53
Subject: Re: [MW:8559] phased array vs. RT

Standards are silent about the replacement of RT by phased array UT.
 
My experience says that you will have to proove and convince your customer / TPI by demenstration that the defect detected by RT is equally detectable by Phased array UT.
 
 Ultimately it would be decision of your customer whether to allow or not...
 
Reg,
Jaydeep Joshi

On Tue, Dec 7, 2010 at 1:30 PM, Navid Navidi <navid_751400@yahoo.com> wrote:
Hi all,

is it possible to use phased array technique instead of RT for NDT teast of a pressure vessels.
Does standard allow us to do so?
what is its advantages?

thank you in advance
Saeed

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.



No virus found in this incoming message.
Checked by AVG - www.avg.com
Version: 9.0.872 / Virus Database: 271.1.1/3301 - Release Date: 12/07/10 01:04:00

No comments:

[MW:34919] Welder qualification certificate

Dear All     anyone can share a format for welder certificate and card format        Thanks & Best Regards Saleem manhappulath Mob:+9665...