what is water break test ?how is it to be perfomed ?for what purpose
is it to be done ?thanks in advance
regards
M.ASLAM

On 12/7/10, mohit arora <mohit2707@gmail.com> wrote:
> Dear,
>
> There can be many reasons for pin holes on top coat.Might be oil
> entraped.Perform Water Break test before Blasting of the surface for better
> results.
>
> On Tue, Dec 7, 2010 at 11:36 AM, Sundaram Sundaram <nss2410@gmail.com>wrote:
>
>> Hi friends,
>> After the finaal coating i have found large number of
>> pin holes on the surface.Can anybody explain what is the reason.
>>
>> with regards & thanks,
>> sundaram
>>
>> --
>> To post to this group, send email to materials-welding@googlegroups.com
>> To unsubscribe from this group, send email to
>> materials-welding+unsubscribe@googlegroups.com<materials-welding%2Bunsubscribe@googlegroups.com>
>> For more options, visit this group's bolg at
>> http://materials-welding.blogspot.com/
>> The views expressed/exchnaged in this group are members personel views and
>> meant for educational purposes only, Users must take their own decisions
>> w.r.t. applicable code/standard/contract documents.
>>
>
>
>
> --
> Regards,
> Mohit Arora,
>
> --
> To post to this group, send email to materials-welding@googlegroups.com
> To unsubscribe from this group, send email to
> materials-welding+unsubscribe@googlegroups.com
> For more options, visit this group's bolg at
> http://materials-welding.blogspot.com/
> The views expressed/exchnaged in this group are members personel views and
> meant for educational purposes only, Users must take their own decisions
> w.r.t. applicable code/standard/contract documents.
>

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34920] Tubesheet Hole step

Hello Team, I have one question any tolerance given for tubesheet Hole step. Please do needful. Regards, AP  -- https://materials-...