Re: [MW:8529] welding inquiry

No you can not....
 
Reason:
1. AWS needs NDE of test coupon before carrying Mechanical unlike ASME
2. Acceptance criteria od NDE and Bend test are stringent in AWS then ASME
3. Difference in the essential variable of AWS and ASME
 
 

Jaydeep Joshi | Welding Engineer. TDW India Limited

Plot No 16 | Phase –III | Alindra – Savli G.I.D.C | Taluka : Savli | Vadodara – 391 775

Board : +91-2667- 619900 | Fax : +91- 2667- 619501| Extension : 7845

E-Mail : jaydeep.joshi@tdwilliamson.com  | www.tdwilliamson.com

Cell: +91 9978959626

P    Before printing, Think about ENVIRONMENTAL responsibility



On Mon, Dec 6, 2010 at 1:35 PM, KASHKOUSHA <kashkousha1@yahoo.com> wrote:

 dear all
can i prepare w.p.s acc.to aws d1.1 with pqr acc.to asme ix
thanks
H.KASHKOUSHA

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34920] Tubesheet Hole step

Hello Team, I have one question any tolerance given for tubesheet Hole step. Please do needful. Regards, AP  -- https://materials-...