RE: [MW:8457] Defect in PQR Specimen

It will be better if you go for a new PQR since you don’t know the exact reason behind the cause of the defects observed in RT film until and unless you do an analysis. May be it could have been done due to wrong parameters selected for welding.

 

Best regards,

 

Shadab Alam Ansari

Welding Engineer

 

cid:image001.gif@01CB80C0.5B165EE0

For Gulf Heavy Industries Co

One of  Al-Bassam Group of Companies

 

Cell Phone No: 00966502090165, Fax No:0096633410105
Telephone No: 0096633400098 (5 Lines) Ext: 232

Email: ansari@ghi.com.sa

Web: "www.ghi.com.sa"

 

Save paper, don't print any emails unnecessarily. Let's save environment for future generation....

 

From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of mahek shah
Sent: Tuesday, November 30, 2010 6:39 PM
To: materials-welding@googlegroups.com
Subject: Re: [MW:8443] Defect in PQR Specimen

 

As defect observed in RT, so pl.rectify the defect with cutting of that portion and again do the welding and than do the heat treatmentagain.And for test piece once u can do the heat treatment only of test piece and again do the heat treatment with product. Than send tht test piece for testing and if it is ok with RT and mechanical testing than we can accept tht.

 

Regards,

 

Mahek shah

L&T 

On Sat, Nov 27, 2010 at 12:30 PM, yoga nandhan <yoganandhan@gmail.com> wrote:

Anyone, Can u plz give your opinion,
 
PQR qualification of SS pipe, 30" x 15.88 mm thik pipe by SMAW+SAW process, In RT defect observed in 200 mm length which is not acceptable as per Sec IX. But rest of the portions are without any significant defects.
 
Can we proceed with the Mechanical testing after discarding the defect area or is it required to Repair & Re-RT to be done in the defect area before taking the specimen for mechancial testing.....  Plz clarify.
 
BR
P.Yoganandhan

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

Comments

Popular posts from this blog

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...

Re: [MW:10788] ON PLOT PIPING & OFF PLOT PIPING

Piping systems involved for the flow lines and gathering lines from the well head isolation valve to the production facility or processing plant isolation valve are determined as OFF PLOT. ON PLOT defines piping system in the processing plant and production platform. ANSI/ASME B31.4 applies for off plot piping system. B31.4 allows the use of either API 1104 or ASME section IX (as appropriate). However, occasionally, a very small system such as piping within 500 feet of a processing plant (some client also said 400 feet) may be declared B31.3 rather than B31.4. When B31.3 is invoked, only ASME Section IX is used. before you decide which code to use for welding procedure and/or welder qualification for pipe welding, you have to know the design and construction code applicable to the system. Please read far enough into scope and diagram illustrating the application of either B31.3 and B31.4 hope this helps rgds 2011/4/21 pradip kumar sil < pradipsil@gmail.com > Dear all, ...