Tuesday, December 14, 2010

[MW:8728] ASME SEC VIII Div 1 1995 Add

Dear All,

How do we get the allowable stress values of plates SA 516 Gr 70
(Normalized) for a vessel constructed according to ASME Sec VIII Div 1
1995ADD?
I need the values for rerating calculations


Regards,


M.Ali

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:35737] Bend Test and Tensile Test failed for ET45 Micro Welded Coupon

Hi As its %elongation is very low  Better try buttering on jt surrace with ductile consumable like pure Ni i. E Ni1 And later weld jt with c...