[MW:8643] Thickness calculation for weldolet

Hi,

How do we calculate the thickness of the weldolet for welding
procedure qualification? Code is B31.3 and ASME SECIX. Weldolet is 8"
SCH40 Bonney forge. So is the thickness (B-C)/2 ie 21mm? Does the
procedure qualification has to support base material thickness of
21mm. The pipe is 8" SCH40. Which section of B31.3 or SEC IX would
address the requirement for this attachment weld between pipe and
weldolet?

Thanks for your help.
Srini

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34920] Tubesheet Hole step

Hello Team, I have one question any tolerance given for tubesheet Hole step. Please do needful. Regards, AP  -- https://materials-...