Thursday, December 9, 2010

[MW:8632] Electrode Qualification Test

Dear all,
 
We want Electrode Qualification Test on Filler wire for MIG ER70S-6 AWS SFA number-5.18
 
Kindly suggest me- what is root gap between & what is the backing plate thickness for 12mm thickness plate.
 


--
Regards,
Pushpraj Anand

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34920] Tubesheet Hole step