[MW:8511] UT or RT for LNG thanks

Good morning for all,

This preocupation is for LNG thanks (120 000 m3 capacity).

As per the contract and procedure, the radiography test (RT) is
required. My contractor needs to do the ultrasonic test (UT).

My question is:
To do the ultrasonic test (UT) or the radiography test (RT)?

Tanks in advance and have a nice day.


Redouane (Project engineer)
Algeria

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34920] Tubesheet Hole step

Hello Team, I have one question any tolerance given for tubesheet Hole step. Please do needful. Regards, AP  -- https://materials-...