Dear Babu,
At present I do not have ABS Spec. But I know that 36 indicate 3600PSI
Yield Strength.

Regards
Israr Ahmed
+919930308261

Kathalingam Babu wrote:
> Hi all
>
> Is anybody have the mechanical properties of Cabon steel (ABS EH36) or any carbon steels , thk greater than 110 mm
>
> The application is Off Shore Structure.
>
> Thanks & Regards,
>
> K. Babu
> Singapore

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34920] Tubesheet Hole step

Hello Team, I have one question any tolerance given for tubesheet Hole step. Please do needful. Regards, AP  -- https://materials-...