[MW:8480] RE: 8478] RE: 8469] Minimum Weld lengh for welder qualification

ASME IX,

 

 

With Kind regards,

S.Elumalai.


From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of Yassein Abdou
Sent: Thursday, December 02, 2010 9:52 AM
To: materials-welding@googlegroups.com
Subject: [MW:8478] RE: 8469] Minimum Weld lengh for welder qualification

 

Dear Eduardo,

                        The code in direct request a qualification for all the circumferential as it will be guide to determine the range qualified on WPQR

 

Best regards, 

Yassein Abdou

Welding & Grating Manager

energya STEEL FABRICATION 

 

 

 

 

 

 


Egypt Factory & Head Office: Industrial Zone A 6 East, 10th of Ramadan City

Tel         +2015 412 239 - 412 249 / +2010 002 0133

Fax        +2015 412 236

Cairo Office: 98 a Hassan Mamoun St. Naser City, Cairo Egypt

Tel         +2 02 22706306 - 2714 631 Fax +2 02 22752 701

KSA Factory: Rabigh - Yanbu High Way Exit 927 Industrial Zone Aramco Road

Tel:         +966 500 150 706 Fax : +966 500 592

Jeddah Office: Haifa Building. King Road  Jeddah City, Saudi Arabia

Tel         +966 2 2907382  Fax +966 2 6882901

www.energyasteel.com     info@energyasteel.com

Personal Mobile: + 2010 0400361     email: yassein.abdou@energyasteel.com

 

 


From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of Eduardo Calva
Sent: Thursday, December 02, 2010 4:39 AM
To: materials-welding@googlegroups.com
Subject: [MW:8469] Minimum Weld lengh for welder qualification

 

Dear friends:
 
Sometimes we have qualified four welders in the same coupon, for example in a 36" Ø pipe coupon the first two  welders apply in overhead position one from 3 to 6 and the other one from 9 to 6, after they finish the cuopon is rotated in order to start the other welder couple as the same process. This has been accepted by our clients but I'd like to know if some code has a minimum lenght to be welded for qualification or it must be the entire cinrcunference of the pipe cuopon to be welded by a welder. I want to be prepared if a client supervisor ask me about it.

Eduardo Calva

QC Coordinator
Global Industries
México.

No comments:

Re: [MW:35289] Welding consumable for S355J2WP material

S355 J2 WP  is a weathering structural steel  It has better atmospheric corrosion resistance. Use E 8018 - W1/W2  Electrodes This is regular...