[MW:8461] Re: RT/UT OF SOCKET WELD/BRANCH WELD

Yes it is common to check 5% or 10% of welds, but 100% RT as specified
in this stnadard is something strange.

On Dec 1, 11:47 am, "paresh k patel" <pkpatel1...@rediffmail.com>
wrote:
> Dear Jignesh
>
> Hi! How are you? Hope fine.
>
> Yes this is carried out to detect gap. In many companies this practice is adopted to verify gap for SW joints.
>
> Regards
>
> Paresh Patel
> ABS IV
>
> On Wed, 01 Dec 2010 07:17:32 +0530  wrote
>
> >Few days ago i came across UOP specification 8-11-12-Piping, which asked radiography of socket / branch welds for low alloy steel/SS. If somebody has done project with UOP in past, pl share their experience.
>
> Also i read one very old B 31.3 Interpretation: 5-13 for the radiography of socket welds as below...
>
> Subject:ANSI/ASME 831.3-1984 Edition, With the ANSI/ASME 831.3a-1984 Addenda, Table 327.4.1A, Limitations on Imperfections in Welds-Internal Porosity 
> Date Issued: December 2, 1986
> Question (1): In ANSI/ASME 831.3, Table 327.4.1 A, under internal porosity forfillet, socket, seal and reinforcement attachment welds, the wording NA (not applicable) is indicated. Does this mean that radiographic examination is not required for this type of joint configuration?
>
> Reply (1): Yes.
> In my opinion, RT of SW is only performed to detect the gap between two components, also in past during some corossion isometric study, we have assigned TML (thikness monitoring location) to carry out RT of SW/BW to confirm the correctness of welded heavy schedule components.
>
> Can any one write few words about the technical feasibility and effectiveness of final result to confirm the soundness of SW/Branch weld by RT/UT with code back up? If somebody have any digital RT film of SW joint pl share.
>
> Best Regds

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:35354] Cast-iron welding

1. Preheat joint area(other area, cover with mineral wool). 2. ENiCi or ENiFe-CI. 3. stringer bead. 4. peening is to be done on weldmetal im...