Saturday, November 27, 2010

Re: [MW:8408] Defect in PQR Specimen

Dear Friend,

There is no any requirement of radiography for PQR test piece in ASME
Section ix. It is our internal test.

It is not code requirement.

See QW-451 for Mechanical Testing

On 11/27/10, yoga nandhan <yoganandhan@gmail.com> wrote:
> Anyone, Can u plz give your opinion,
>
> PQR qualification of SS pipe, 30" x 15.88 mm thik pipe by SMAW+SAW process,
> In RT defect observed in 200 mm length which is not acceptable as per Sec
> IX. But rest of the portions are without any significant defects.
>
> Can we proceed with the Mechanical testing after discarding the defect area
> or is it required to Repair & Re-RT to be done in the defect area before
> taking the specimen for mechancial testing..... Plz clarify.
>
> BR
> P.Yoganandhan
>
> --
> To post to this group, send email to materials-welding@googlegroups.com
> To unsubscribe from this group, send email to
> materials-welding+unsubscribe@googlegroups.com
> For more options, visit this group's bolg at
> http://materials-welding.blogspot.com/
> The views expressed/exchnaged in this group are members personel views and
> meant for educational purposes only, Users must take their own decisions
> w.r.t. applicable code/standard/contract documents.
>


--
Regards,
Shaunak Upadhyay,
e-mail: skupadhyay@nuberg.in
Mo:- 09662519411

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...