Friday, November 26, 2010

Re: [MW:8390] SS 304 to SS 321 welding

You need to weld with FW ER347 or Electrode E347-15/16
Regards
Aarpee

On Thu, Nov 25, 2010 at 6:45 PM, <hrishikm07@gmail.com> wrote:
1.Pl advise if SS 304 to SS 321 piping welding is possible? If so what is the consumable to be used
2. Is welding of SS 321 possible with E 308 consumable provided one has an approved WPS/PQR?

Thanks
Hrishi
Sent on my BlackBerry® from Vodafone

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...