Re: [MW:8345] Regarding UT of weld

Dear Mr. Yogesh....Question is not related to UT of plates...its related to UT of Butt joints for 8 mm plates.....


Please Suggest....wether it is to be done or not.

On Sun, Nov 21, 2010 at 9:30 PM, Yogesh kumar <yogeshandpini@gmail.com> wrote:
Sahu Sir

As per asme sec v,for fully killed steel,UT is to be done on thickness 13mm and above.

regards

yogesh







On Sat, Nov 20, 2010 at 9:14 AM, kamaleshwar sahu <kamaleshwar.sahu@beekaycorp.com> wrote:
Dear all,
             Please suggest me for UT of butt weld joint mat. A516 to A516 and thickness is 08 mm, wether it is to be done or not.
 
Regards

Kamaleshwar Kumar Sahu
AGM(QA&I)
Cell: +91 97520 99054
bk.gif
BEEKAY ENGINEERING CORPORATION
45/47, Industrial Estate, Bhilai (C.G.), INDIA
Tel: +91 788 4082240 (D) /4082200
Fax: +91 788 4082288/99
E-Mail: kamaleshwar.sahu@beekaycorp.com
Web: www.beekaycorp.com

iso9001.gif iso.gif ohsas.gif
P Please consider the environment before printing my email

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...