Monday, November 1, 2010

RE: [MW:7985] Percentage for N.D.T.

Min requirement will be as per para 341.4 of B31.3, based fluid category (e.g. normal – 5%, severe cyclic-100%). This will be extended by designers based on MOC. Fluid, design conditions etc.

 

From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of john clough
Sent: Monday, November 01, 2010 12:11 PM
To: materials-welding
Subject: [MW:7984] Percentage for N.D.T.
Importance: High

 

Sirs
Could you tell me where to find the percentage for N.D.T. using ASME B31-3 for example.
If working on a project where there is no client specification which states the percentages but working to ASME where would I find the percentage for radiography for example, I have seen an old ANSI Specification which did include the percentages but to my knowledge not in ASME.
If there is no guide lines for N.D.T. percentage in ASME then is there any way to calculate using pressure, material and the chemical which the pipe will be used for. 
 
Best Regards
 
John


No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...