Tuesday, November 30, 2010

[MW:8449] EEMUA 158

Hi All

Can u pls guide me which section of EEMUA 158 :1994 gives details of the positions and progressions qualified by welding 2G & 3G , UPHILL? Please quote the reference paragraph number from the standard.

Also where can I find the values for interpass temperature in the standard? (5.3.3 is clear about preheat, but does not gives much details about interpass temperature, the material is carbon steel, CE:m 0.46,)

BR

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...