Hi,
You can go for coating thickness gauge.
www.oxford-instruments.com (http://www.oxford-instruments.com/products/coating-thickness/coating-gauges/Pages/coating-gauges.aspx)

Thanks & Regards,

(Karthik)

Karthikeyan.S
QA/QC Manager
Getabec Energy Co.,Ltd.
379,Moo6,Soi8,Nikhomphatana,
Rayong-21180,
Thailand.
Phone: 0066 38 897035-8 (Off)
Fax: 0066 38 897034
Hand Phone: 0066 892512282


--- On Tue, 11/30/10, Noushad cp <ncp.clt@gmail.com> wrote:

From: Noushad cp <ncp.clt@gmail.com>
Subject: ENP Measurement
To: "materials-welding" <materials-welding@googlegroups.com>
Cc: "Karthik" <karthik6684@yahoo.com>
Date: Tuesday, November 30, 2010, 2:42 PM

Dear All,


How to measure Electroless Nickel Plating (Coating) ?i would like to know the Instrument which is use for ENP Measurement.


Thanks and Regards,


Noushad

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...