Monday, November 29, 2010

[MW:8429] RE: 8396] Excess Weld Root Penetration-Reg.

Hi,

 

We can  measure and making bench mark for Root penetration on the basis of Radiographs in the field of Pipe Line Welding by using LP /EP penny.

 

Regards

M.Nagoor Meeran

KKNPP-Project

Kudankulam-627106

Tamilnadu.

 

 

From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of muthu kumaran
Sent: Saturday, November 27, 2010 10:24 AM
To: materials-welding@googlegroups.com
Subject: [MW:8396] Excess Weld Root Penetration-Reg.

 

Hi,

 

How to measure and making bench mark for Root penetration on the basis of Radiographs in the field of Pipe Line Welding.

--
Cordially,

P.Muthukumaran
Welding Inspector

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...