[MW:8405] Electrode Selection for X60/F60 Material

Team,


While reviewing a WPS/PQR we have following details

Material to be welded using the below detailed WPS is : A694 F60

The WPS& PQR is qualified with SA 350 LF2 materiaal with following
consumables
ER 70S3 -Root
E 7018 H4 -Hot pass
EH12K - Fill& Cap
Applicable code ASME Sec-IX & ASME B 31.3
Here my question is
material to be welded is A694 F60 which is having Tensile strength of
75 KSI .The consumable is used in the PQR is not matching the strength
level hence i'm not satisfied with this selection.
My opinion is to use ER 80S3,E 8018 & EH12K.
Dear memebers please provide your inputs.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...