Hi Gents,

I have  doubt reg HOT PASS.

1. what is the purpose of doing HOT PASS with more speed and high current?

2. Should the Welding Process used for Root be the same for HOT PASS? If not necessarily then how should we decide?

Thank you All

Regards,

Vasu


--