Wednesday, November 24, 2010

[MW:8365] pwht thickness as per AWS D1.1

Hi,
As per ASME B31.3 above 20mm thickness materials we are doing pwht.As per AWS D1.1, above which thickness we need to carryout pwht.???

Thanks & Regards
Mijin
Mumbai

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.