Saturday, October 30, 2010

Re: [MW:7936] golden weld joint require ments

Mr Gulam

 

I could remember the following things for Golden weld.

 

a) It means , other than of fabrication shop welding, the balance welding which will  be done with only one joint at site welding( or) in a tie -in work process. This type of joints are confirmed by 100% RT or UT (NDT), since there may be  a practice problem in the hydro test depends with the pipe  length.

 

b)There is no specific code for Golden joint but most of the companies are follow  to perform a "golden weld", with 100% NDT by eliminating hydro test.

 

c) We can refer  ASME 31.4, and  it  permits a "waiver" of a hydro test on "tie-in" welds between two sections of piping , that the weld has already undergone 100% NDT (see Section 437.1.4 (b) Testing Tie ins, ASME B31.4 2002 Edition).

 

T.Mahendran
KSA

 


From: Gulam kader <armvasi@gmail.com>
To: materials-welding@googlegroups.com
Sent: Sat, October 30, 2010 9:42:49 AM
Subject: [MW:7933] golden weld joint require ments

Dear all,

can any one explain the golden joint welding , NDT and inspection requirement with Code references.

Regards,

Gulam Kader

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments: